Advanced low dielectric constant organosilicon plasma chemical vapor deposition films
Abstract
A porous low k or ultra low k dielectric film comprising atoms of Si, C, O and H (hereinafter “SiCOH”) in a covalently bonded tri-dimensional network structure having a dielectric constant of less than about 3.0, a higher degree of crystalline bonding interactions, more carbon as methyl termination groups and fewer methylene, —CH 2 — crosslinking groups than prior art SiCOH dielectrics is provided. The SiCOH dielectric is characterized as having a FTIR spectrum comprising a peak area for CH 3 +CH 2 stretching of less than about 1.40, a peak area for SiH stretching of less than about 0.20, a peak area for SiCH 3 bonding of greater than about 2.0, and a peak area for Si—O—Si bonding of greater than about 60%, and a porosity of greater than about 20%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A dielectric material comprising atoms of Si, C, O and H and having a tri-dimensional network structure in which the material has a FTIR spectrum comprising a peak area for CH 3 +CH 2 stretching of less than about 1.40, a peak area for SiH stretching of less than about 0.20, a peak area for SiCH 3 bonding of greater than about 2.0, and a peak area for Si—O—Si bonding of greater than about 60.
- Claim 2Depends on #1
The dielectric material of claim 1 wherein said material has a dielectric constant of less than about 3.0.
- Claim 3Depends on #2
The dielectric material of claim 2 wherein said dielectric constant is in a range from about 2.2 to about 2.8.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (4)
- U.S. Appl. No. 10/390,801, Ultra Low K (ULK) SiCOH Film And Method, Stephen M. Gates, et al., filed Mar. 18, 2003.
- U.S. Appl. No. 10/709,320, LowK Interlevel Dielectric Layer (ILD) And Method, Jia Lee, et al., filed Apr. 28, 2004.
- U.S. Appl. No. 10/758,724, "Low K And Ultra Low K SiCOH Dielectric Films And Methods To Form The Same", Stephen M. Gates, et al., filed Jan. 16, 2004.
- U.S. Appl. No. 10/964,254, "Ultra Low k Plasma Enhanced Chemical Vapor Deposition Processes Using A Single Bifunctional Precursor Containing Both A SiCOH Matrix Functionality And Organic Porogen Functionality", Son Nguyen, et al., filed Oct. 13, 2004.