Patents
US 8,932,674 B2#43707179 Most CitedActiveUnited States (USPTO)Utility

Vapor deposition methods of SiCOH low-k films

2Forward Citations (#43707179 Global)
0.2/yrCitation Velocity (#35796979 Global)
0.92Citation PageRank (#46357448 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed are precursors that are adapted to deposit SiCOH films with dielectric constant and Young's Modulus suitable for future generation dielectric films.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a SiCOH film layer on a substrate, the method comprising the steps of: providing a reaction chamber having at least one substrate disposed therein; introducing into the reaction chamber a Si—(CH 2 ) n —Si containing precursor, with n=1 or 2, selected from the group consisting of: wherein each of R1 through R4 is independently selected from the group consisting of H, methyl, ethyl, propyl, vinyl, and C1-C3 alkoxy; R5 is selected from the group consisting of methyl, ethyl, and propyl; introducing into the reaction chamber a vinyl-containing precursor having the formula Si(R1)

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP H0324093 ATrialkylsilylmethyl group-containing silane compound—13
US 5,296,624 APreparation of sterically-hindered organosilanes199430
US 5,989,998 AMethod of forming interlayer insulating film1999213
US 6,159,871 AMethod for producing hydrogenated silicon oxycarbide films having low dielectric constant2000271
US 6,312,793 B1Multiphase low dielectric constant material2001282
US 6,410,151 B1Composition for film formation, method of film formation, and insulating film200230
US 6,479,110 B2Multiphase low dielectric constant material and method of deposition2002144
US 6,558,747 B2Method of forming insulating film and process for producing semiconductor device200319
US 6,583,048 B2Organosilicon precursors for interlayer dielectric films with low dielectric constants2003144
WO 2004/049422 A1Insulating film material containing organic silane or organic siloxane compound, method for producing same, and semiconductor device—3
US 6,756,323 B2Method for fabricating an ultralow dielectric constant material as an intralevel or interlevel dielectric in a semiconductor device200447
US 6,797,643 B2Plasma enhanced CVD low k carbon-doped silicon oxide film deposition using VHF-RF power200422
WO 2004/083495 A2Ultra low k (ulk) sicoh film and method—25
JP 2004288979 AMethod for forming insulating film—7
US 2004241463 A1Mechanical enhancer additives for low dielectric films—29
US 6,846,515 B2Methods for using porogens and/or porogenated precursors to provide porous organosilica glass films with low dielectric constants2005117
US 2005113472 A1Porous materials—32
WO 2005/080629 A2SILICON COMPOUNDS FOR PRODUCING SiO2-CONTAINING INSULATING LAYERS ON CHIPS—6
US 2005194619 A1SiCOH dielectric material with improved toughness and improved Si-C bonding, semiconductor device containing the same, and method to make the same—69
US 2005196974 A1Compositions for preparing low dielectric materials containing solvents—35
US 6,953,984 B2Hydrogenated oxidized silicon carbon material200515
US 2005260420 A1Low dielectric materials and methods for making same—29
JP 2006040936 AMethod and apparatus of depositing insulating film—5
US 2006079099 A1Ultra low k plasma enhanced chemical vapor deposition processes using a single bifunctional precursor containing both a SiCOH matrix functionality and organic porogen functionality—65
US 7,030,468 B2Low k and ultra low k SiCOH dielectric films and methods to form the same200668
JP 2006111738 AComposition for surface hydrophobizing, surface hydrophobizing method, semiconductor device and its manufacturing method—5
US 7,049,247 B2Method for fabricating an ultralow dielectric constant material as an intralevel or interlevel dielectric in a semiconductor device and electronic device made200632
US 7,049,427 B2Genetic sequences encoding dominant-negative chalcone synthase and uses therefore20067

Non-Patent Literature (5)

  • "Silicon compounds: silanes and silicones," 2nd ed., Barry Arkles and Gerald Larson, eds., Gelest, Inc., Morrisville, PA, 2008, p. 484.
  • "The International Technology Roadmap for Semiconductors", 2007, Interconnect.
  • Air Liquide, "Development of low-k precursors for next generation IC manufacturing," poster session of Advanced Metallization Conference 2010, Oct. 5-7, 2010, Albany, New York, accessed at http://www.sematech.org/meetings/archives/3d/8964/index.htm, 1 pg.
  • Anonymous, "Low-k precursors adapted for incorporation of porosity," http://www.ip.com, No. IPCOM000185211D, published Jul. 15, 2009.
  • Austrian Search Report and Written Opinion for corresponding SG 201205981-2, Mar. 7, 2014.