Method for fabricating an ultralow dielectric constant material

25Forward Citations (#3095414 Global)
1.1/yrCitation Velocity (#5473049 Global)
2.59Citation PageRank (#9579830 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for fabricating a thermally stable ultralow dielectric constant film comprising Si, C, O and H atoms in a parallel plate chemical vapor deposition process utilizing plasma enhanced chemical vapor deposition (“PECVD”) process is disclosed. To enable the fabrication of thermally stable ultralow dielectric constant film, specific precursor materials are used, such as, cyclic siloxanes and organic molecules containing ring structures, for instance, tetramethylcycloterasiloxane and cyclopentene oxide. To stabilize plasma in the PECVD reactor and thereby improve uniformity of the deposited film, CO 2 is added to TMCTS as a carrier gas, or CO 2 or a mixture of CO 2 and O 2 are added to the PECVD reactor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 25.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a thermally stable ultralow dielectric constant film comprising the steps of: providing a plasma enhanced chemical vapor deposition (PECVD) reactor; positioning a substrate in said PECVD reactor; flowing a first precursor gas comprising cyclic siloxane molecules into said PECVD reactor; flowing at least a second precursor gas comprising organic molecules with ring structures having C, H and O atoms into said PECVD reactor;and depositing a film comprising Si, C, O and H and a multiplicity of nanometer-sized pores on said substrate in presence of CO 2 or CO 2 and O 2 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 25 total)

PatentTitleYearCitations
US 2008026203 A1ULTRA LOW K (ULK) SiCOH FILM AND METHOD—14
US 7,494,938 B2Advanced low dielectric constant organosilicon plasma chemical vapor deposition films20095
US 2006183345 A1Advanced low dielectric constant organosilicon plasma chemical vapor deposition films—25
US 2009146265 A1ULTRA LOW k PLASMA ENHANCED CHEMICAL VAPOR DEPOSITION PROCESSES USING A SINGLE BIFUNCTIONAL PRECURSOR CONTAINING BOTH A SiCOH MATRIX FUNCTIONALITY AND ORGANIC POROGEN FUNCTIONALITY—5
US 8,097,932 B2Ultra low κ plasma enhanced chemical vapor deposition processes using a single bifunctional precursor containing both a SiCOH matrix functionality and organic porogen functionality20120
US 8,101,236 B2Method of fabricating a SiCOH dielectric material with improved toughness and improved Si-C bonding20128
US 2004038545 A1Plasma processes for depositing low dielectric constant films—9
US 7,892,648 B2SiCOH dielectric material with improved toughness and improved Si-C bonding20117
US 2007128882 A1Advanced low dielectric constant organosilicon plasma chemical vapor deposition films—2
US 2009297823 A1ULTRA LOW K (ULK) SiCOH FILM AND METHOD—4
US 2007228570 A1RELIABLE BEOL INTEGRATION PROCESS WITH DIRECT CMP OF POROUS SiCOH DIELECTRIC—19
US 2005276930 A1Ultra low K (ULK) SiCOH film and method—25
US 2006166491 A1Dual damascene interconnection having low k layer and cap layer formed in a common PECVD process—7
US 2011101489 A1SiCOH DIELECTRIC MATERIAL WITH IMPROVED TOUGHNESS AND IMPROVED Si-C BONDING, SEMICONDUCTOR DEVICE CONTAINING THE SAME, AND METHOD TO MAKE THE SAME—7
US 2009093130 A1Silicon oxycarbide, growth method of silicon oxycarbide layer, semiconductor device and manufacture method for semiconductor device—1