US 6,918,968 B2#5576978 Most CitedExpiredUnited States (USPTO)Utility

Austenitic stainless steel

16Forward Citations (#5576978 Global)
0.8/yrCitation Velocity (#9767637 Global)
4.70Citation PageRank (#3666140 Global)
18Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An austenitic stainless steel excellent in high temperature strength, high temperature ductility and hot workability, consisting of, by mass %, C: more than 0.05% to 0.15%, Si: 2% or less, Mn: 0.1 to 3%, P: 0.04% or less, S: 0.01% or less, Cr: more than 20% to less than 28%, Ni: more than 15% to 55%, Cu: more than 2% to 6%, Nb: 0.1 to 0.8%, V: 0.02 to 1.5%, sol. Al: 0.001 to 0.1%, but sol.Al≦0.4×N, N: more than 0.05% to 0.3% and O (Oxygen): 0.006% or less, but O≦1/(60×Cu), and the balance Fe and impurities. The austenitic stainless steel may contain at least one of Co, Mo, W, Ti, B, Zr, Hf, Ta, Re, Ir, Pd, Pt and Ag, and/or at least one of Mg, Ca, Y, La, Ce, Nd and Sc.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 16.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An austenitic stainless steel characterized by consisting of, by mass %, C: more than 0.05% to 0.15%, Si: 2% or less, Mn: 0.1 to 3%, P: 0.04% or less, S: 0.01% or less, Cr: more than 20% to less than 28%, Ni: more than 15% to 55%, Cu: more than 2% to 6%, Nb: 0.1 to 0.8%, V: 0.02 to 1.5%, sol.Al: 0.001 to 0.1%, N: more than 0.05% to 0.3% and O (Oxygen): 0.006% or less, and the balance Fe and impurities, further characterized by satisfying the following formulas (1) and (2): P≦1/(11×Cu)  (1) sol.Al≦0.4×N  (2) wherein each element symbol in the formulas (1) and (2) represents the content (mass %)

  2. Claim 2Independent Claim

    An austenitic stainless steel characterized by consisting of, by mass %, C: more than 0.05% to 0.15%, Si: 2% or less, Mn: 0.1 to 3%, P: 0.04% or less, S: 0.01% or less, Cr: more than 20% to less than 28%, Ni: more than 15% to 55%, Cu: mo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 16 total)

PatentTitleYearCitations
RU 2,635,645 C1Steel20170
US 8,506,729 B2Austenite-type stainless steel hot-rolling steel material with excellent corrosion resistance, proof-stress, and low-temperature toughness and production method thereof20131
US 2006243356 A1Austenite-type stainless steel hot-rolling steel material with excellent corrosion resistance, proof-stress, and low-temperature toughness and production method thereof—12
US 2008107559 A1Austenitic stainless steel—32
US 7,866,199 B2Method for manufacturing seamless steel pipe made of high Cr-high Ni alloy steel20114
RU 2,651,069 C1Iron-based alloy20180
US 9,150,947 B2Austenitic stainless steel20154
US 2010034689 A1Austenitic stainless steel—24
US 9,347,121 B2High strength, corrosion resistant austenitic alloys20166
US 8,105,447 B2Austenitic stainless hot-rolled steel material with excellent corrosion resistance, proof stress, and low-temperature toughness20123
US 2012111457 A1Austenite-type stainless steel hot-rolling steel material with excellent corrosion resistance, proof-stress, and low-temperature toughness and production method thereof—0
US 2011067475 A1Process for Producing High-Alloy Seamless Tube—7
US 10,174,397 B2Titanium-free alloy20194
US 2010230011 A1Austenite-type stainless steel hot-rolling steel material with excellent corrosion resistance, proof-stress, and low-temperature toughness and production method thereof—2
US 2010000281 A1Method for manufacturing seamless steel pipe made of high Cr-high Ni alloy steel—2