Abstract

An austenitic stainless steel hot-rolled steel material can be provided which has sea-water resistance and strength superior to conventional steel. Low-temperature toughness can be maintained, which is preferable in a structural member of speedy craft. The steel material can include an austenitic stainless steel hot-rolled steel material which excels in the properties of corrosion resistance, proof stress, and low-temperature toughness. In such austenitic stainless steel hot-rolling steel material, e.g., PI [=Cr+3.3(Mo+0.5W)+16N] ranges from 35 to 40, δ cal [=2.9(Cr+0.3Si+Mo+0.5W)−2.6(Ni+0.3Mn+0.25Cu+35C+20N)−18] ranges from −6 to +2, and a 0.2% proof stress at room temperature is not less than 550 MPa, Charpy impact value measured using a V-notch test piece at −40° C. is not less than 100 J/cm2, and the pitting potential measured in a deaerated aqueous solution of 10% NaCl at 50° C. (Vc′100) is not less than 500 mV (as it relates to saturated Ag/AgCl).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An austenitic stainless hot-rolled steel material having a superior corrosion resistance, a proof stress, and a low-temperature toughness, wherein a content of intermetallic compounds contained in the steel material is at most about 0.5 mass %, about 0.2% proof stress at a room temperature is at least about 550 MPa, a Charpy impact value measured using a V-notch test piece at about −40° C. is at least about 100 J/cm 2 , a pitting potential measured in a deaerated aqueous solution of about 10% NaCl at about 50° C. (Vc′100) is at least about 500 mV as compared to a saturated solution of Ag/AgCl,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • English-hand translation of Japanese patent No. 359006359, Oomura, Sadafumi et al., Jan. 13, 1984.