Austenitic steel having improved high-temperature strength and corrosion resistance
Abstract
An austenitic steel having improved high-temperature strength as well as corrosion resistance is disclosed. The steel consists essentially of, by weight %: C: not more than 0.15%, Si: not more than 1.0%, Mn: not more than 10%, Cr: 20-30%, Ni: 30-55%, at least one of Mg and Ca in a total amount of 0.0010-0.0500%, Mo: 0.5-6.0% and/or W: 1.0-12.0%, wherein Mo(%)+1/2W(%)=0.5-6.0(%), B: 0-0.0100%, Zr: 0-0.200%, Ti: 0-0.30%, Nb: 0-1.00%, V: 0-1.00%, and balance: Fe and incidental impurities, of which impurities P, S, and Al are restricted to: P: not more than 0.020%, S: not more than 0.010%, and Al: not more than 0.030%, P (%)+S (%)+Al (%) being less than 0.050%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 16.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
An alloy having improved high-temperature strength and corrosion resistance, which consists essentially of, by weight %: C: not more than 0.15%; Si: not more than 1.0%; Mn: not more than 10%; Cr: 20-30%; Ni: 30-55%; at least one of Mg and Ca in a total amount of 0.0010-0.0500%; W: 1.0-12.0%; either B: 0.0010-0.0100% and Zr: 0.005-0.200% or B=0.0010-0.0100%; with the balance being: Fe and incidental impurities, of which impurities P, S, and Al are restricted to: P: not more than 0.020%; S: not more than 0.010%; and Al: not more than 0.030% wherein P(%)+S(%)+Al(%) is less than 0.050%.
- Claim 2Depends on #1
An alloy as defined in claim 1, which consists essentially of, by weight %: C: not more than 0.15%; Si: not more than 1.0%; Mn: not more than 10%; Cr: 20-30%, Ni: 30-55%; at least one of Mg and Ca in a total amount of 0.0010-0.0500%; W: 1.0-12.0%;