Patents
US 6,818,294 B2#16886081 Most CitedExpiredUnited States (USPTO)Utility

Polyoxymethylene fiber and method for production thereof

6Forward Citations (#16886081 Global)
0.3/yrCitation Velocity (#27346757 Global)
2.00Citation PageRank (#14545159 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Polyoxymethylene fiber having a high strength and a high modulus of elasticity is provided. Polyoxymethylene fiber comprising polyoxymethylene copolymer having a half-crystallization time of at least 30 sec, when the polyoxymethylene copolymer is cooled from a melted state at 200° C. to 150° C. at a cooling speed of 80° C./min and maintained constantly at the temperature of 150° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Polyoxymethylene fiber comprising a polyoxymethylene copolymer that has a half-crystallization time of at least 30 sec when the polyoxymethylene copolymer is cooled from a molten state at 200° C. to 150° C. at a cooling rate of 80° C./min and maintained constantly at the temperature of 150° C.

  2. Claim 2Depends on #1

    The polyoxymethylene fiber as described in claim 1 wherein the half-crystallization time of the polyoxymethylene copolymer is at least 100 sec.

  3. Claim 3Depends on #1

    The polyoxymethylene fiber as described in claim 1 wherein the polyoxymethylene copolymer contains repeating units of oxyalkylene represented by the following formula (1) in repeating units of oxymethylene: -[-(CH 2 ) n -O-] m   (1) (In the formula, n represents an integer of two or more; and m is an integer of one

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗