Polyoxymethylene fibers, production thereof and use thereof
Abstract
Described are fibers comprising a polyoxymethylene copolymer having an ISO 1133 MVR melt index (determined at 190° C. under a load of 2.16 kg) in the range from 0.3 to 30 ml/10 min which possess a bend recovery (measured by the double loop method in air and/or water) of not less than 125° C. These fibers are useful in brushes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Fibers comprising a polyoxymethylene copolymer having an ISO 1133 MVR melt index (determined at 190° C. under a load of 2.16 kg) in the range from 0.3 to 30 ml/10 mm which possess a bend recovery (measured by the double loop method in air and/or water) of not less than 125° C.
- Claim 2Depends on #1
The fibers according to claim 1 wherein the polyoxymethylene copolymer has a melting point of not less than 140° C. and a weight average molecular weight M w in the range from 5000 to 200 000.
- Claim 3Depends on #1
The fibers according to claim 1 wherein the polyoxymethylene copolymer has an MVR value (190/2.16) in the range from 1 to 10 ml/10 min.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗