Process for melt spinning polyoxymethylene filaments having elastic recovery
Abstract
A process for producing filamentary material of an oxymethylene polymer having an elastic recovery at 70* F. of at least about 70 percent when subjected to a strain of up to 50 percent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 13.
Claims (3 — 0 Independent, 3 Dependent)
- Claim 2Depends on #1
The process of claim 1 comprising subjecting the random oxymethylene copolymer filamentary material to a quench temperature up to about 285* F., a first after-stretching operation at a draw ratio of from about 1.3 to 1.5 and a second after-stretching operation at a draw ratio of from about 1.3 to 1.5.
- Claim 3Depends on #1
The process of claim 1 comprising initially taking up the random oxymethylene copolymer filamentary material at a drawdown ratio of from about 25 to 350, continuously advancing said material at a point beyond the point of initial takeup at a rate greater than that of said takeup such that said fully solidified material is drawn at a temperature of from about 50* F. to 250* F. and a draw ratio of from about 1.2 to 2.3
- Claim 4Depends on #1
The process of claim 1 comprising taking up the filamentary material just subsequent to extrusion at an overall drawdown ratio
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.