Patents
US 5,770,113 A#7618698 Most CitedExpiredUnited States (USPTO)Utility

Zinc oxide ceramics and method for producing the same

13Forward Citations (#7618698 Global)
0.5/yrCitation Velocity (#17721872 Global)
2.42Citation PageRank (#10740080 Global)
16Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Zinc oxide ceramics and a method for producing the same are provided wherein zinc oxide varistors for low and high voltages having excellent electric characteristics and high reliability upon DC loading and surge can be obtained in high yield by low-temperature sintering. 0.2 to 20 parts by weight of a mixed powder of bismuth oxide, titanium oxide and antimony oxide is treated in advance at a temperature of 850 DEG C. or less. The synthetic powder thus obtained is added to 100 parts by weight of ZnO material powder to produce ceramics. By using the ceramics for a zinc oxide varistor, a zinc oxide varistor for a low or high voltage can be produced in high yield, which can be sintered at a low temperature and is excellent in electric characteristics and reliability upon DC loading and surge. Aluminum is sprayed on both sides of a sintered body so that an aluminum layer is formed. Copper is sprayed on the aluminum layer so that an electrode is formed. A lead wire is bonded to the electrode. Then, portions of the molded bodies other than the lead wire are coated and insulated so that the zinc oxide varistor can be obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 13.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a zinc oxide ceramic, comprising: preparing a composition comprising: 100 parts by weight of zinc oxide as a first component; 0.1 to 5.0 parts by weight of at least one of cobalt oxide and manganese oxide as a second component; and 0.2 to 20 parts by weight of a powder mixture of oxides of bismuth, titanium and antimony as a third component; and sintering the composition, wherein the powder mixture is heated at temperature of 450° to 800° C. before the composition is formed.

  2. Claim 2Independent Claim

    Method for producing a zinc oxide ceramic, comprising: preparing a composition comprising zinc oxide as a first component, at least one of cobalt oxide and manganese oxide as a second component, and a mixed powder of oxides of bismuth, titanium, antimony, chromium and boron; and sintering the composition, wherein the mi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • "Grain growth processes in ZnO varistors with various valence states of managanese and cobalt", Ying-Chung Chen et al., Japanese Journal of Applied Physics, vol. 69, No. 12, Jun. 15, 1991, pp.l 8363-8367.
  • "Nonohmic Properties of Zinc Oxide Deramics", Michio MATUOKA, Japanese Journal of Applied Physics, vol. 10, No. 65, Jun. 1971, pp. 736-746.
  • Grain growth processes in ZnO varistors with various valence states of managanese and cobalt , Ying Chung Chen et al., Japanese Journal of Applied Physics, vol. 69, No. 12, Jun. 15, 1991, pp.l 8363 8367.
  • Nonohmic Properties of Zinc Oxide Deramics , Michio MATUOKA, Japanese Journal of Applied Physics, vol. 10, No. 65, Jun. 1971, pp. 736 746.