Patents
US 4,094,061 A#855822 Most CitedExpiredUnited States (USPTO)Utility

Method of producing homogeneous sintered ZnO non-linear resistors

52Forward Citations (#855822 Global)
1.1/yrCitation Velocity (#5889443 Global)
20.73Citation PageRank (#314420 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of making a homogeneous ZnO sintered resistor body, having a substantially uniform density, which can exhibit non-linear V-I characteristics by a bulk effect, comprises the steps of: (1) mixing about 75 mole % to about 98 mole % of small, finely divided, solid ZnO and about 2 mole % to about 25 mole % of at least one small, finely divided, solid additive effective to produce non-linear characteristics within the body, preferably one or more oxides selected from the group consisting of TiO 2 , Ta 2 O 5 , FeO, In 2 O 3 , B 2 O 3 , Al 2 O 3 , SnO 2 , Sn 3 O 4 , Mo 2 O, SiO 2 , BaO, SrO, PbO, NiO, CaO, MgO, Bi 2 O 3 , Co 3 O 4 , CoO, MnO, MnO 2 , Cr 2 O 3 , and Sb 2 O 3 , with an aqueous binder solution comprising a fugitive organic, water soluble binder, wherein the weight ratio of the aforesaid mixed finely divided solids:binder is between about 100:1 to about 100:10, to provide a slurry; (2) simultaneously drying, mixing and agglomerating the slurried solids into a mass of larger substantially spherical particles containing the finely divided solids and binder; (3) pressing a mass of the agglomerated particles or powder in a uni-axial press, to provide a cohesive pressed gr

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 52.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a homogeneous, sintered, resistor body, having a substantially uniform density, which can exhibit nonlinear V-I characteristics, comprising the steps of: (A) mixing: (1) a solid particle composition admixture of 75 mole % to 98 mole % of small, finely divided ZnO and 2 mole % to 25 mole % of a small, finely divided additive compound effective to produce non-linearity characteristics within the body, with (2) an aqueous binder solution comprising an organic, water soluble binder that will decompose at temperatures of between about 150° to about 600° C leaving no carbon resi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Kingery, Ceramic Fabrication Processes, pp. 64-70, 1958.