Abstract

A method of making a ZnO powder composition, which can exhibit non-linear V-I characteristics, comprises the steps of: (1) mixing about 75 mole % to about 98 mole % of small, finely divided, solid ZnO and about 2 mole % to about 25 mole % of at least one small, finely divided, solid additive oxide effective to produce nonlinear characteristics, with an aqueous binder solution comprising an organic, water soluble fugitive binder, to provide a slurry; (2) simultaneously drying, mixing and agglomerating the slurried solids into a mass of larger substantially spherical particles containing the finely divided solids and binder; (3) pressing a mass of the agglomerated particles, to provide a cohesive pressed green body; and then (4) heating the pressed body, first at a temperature rate increase effective to slowly decompose and remove the fugitive binder from the body and then heating at a temperature of between 1,050 DEG C. to about 1,400 DEG C. for a time effective to sinter together the particles of the body, forming ZnO grains; (5) crushing the sintered body to provide finely divided powder particle fragments; (6) passing the particle fragments through a means to measure particle siz

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 33.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a ZnO powder composition, which can exhibit non-linear V-I characteristics, comprising the steps of: (1) mixing: (a) 75 mole % to 98 mole % of finely divided, ZnO particles and 2 mole % to 25 mole % of finely divided, additive particles effective to produce non-linear V-I characteristics, with (b) an aqueous binder solution comprising an organic, water soluble binder that will decompose at temperatures of between about 150° C. and 600° C., to provide a mixed particle-binder slurry, and then (2) simultaneously dry, mix, agglomerating the slurry to form a mass of larger

Technical Overview & Description