Patents
US 5,459,201 A#3687973 Most CitedExpiredUnited States (USPTO)Utility

Impact strength, stress-whitening and bruise-resistance for impact modified polypropylene

22Forward Citations (#3687973 Global)
0.7/yrCitation Velocity (#10592832 Global)
3.47Citation PageRank (#6001012 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a process for preparing high melt flow rate thermoplastic compositions that have improved impact and bruise-resistance properties and to the thermoplastic composition that are produced by the process of the instant invention. Specifically, the process comprises the steps of precontacting a non-crosslinked elastomeric polymeric component with a peroxide compound at a temperature below the decomposition temperature of the peroxide and below the melting point of the non-crosslinked polymeric component to produce a peroxide adsorbed polymeric component; and melt mixing the aforementioned peroxide adsorbed polymeric component with a high propylene content polymeric component selected from the group consisting of homopolymers of propylene, block copolymers of propylene and ethylene, and thermoplastic olefin polymers at a temperature above the decomposition temperature of the peroxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a high melt flow rate thermoplastic polymeric composition having improved dynamic melt rheological properties comprising the steps of: (a) forming a peroxide absorbed composition consisting of a non-crosslinked elastomeric component and a peroxide compound by precontacting said non-crosslinked elastomeric component with said peroxide compound at a temperature below the decomposition temperature of the peroxide and below the melting point of the non-crosslinked elastomeric component; and (b) melt mixing the peroxide absorbed composition of step (a) with a high propylen

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,240,727 AProcess for preparing cellular bodies from mixes containing amorphous polypropylene and expanded materials obtained therefrom196612
US 3,456,038 ABlends of ethylene-propylene rubber and atactic polypropylene196910
US 3,758,643 AD polyolefin plastic thermoplastic blend of partially cured monoolefin copolymer rubber an1973155
US 3,806,558 ADynamically partially cured thermoplastic blend of monoolefin copolymer rubber and polyolefin plastic1974256
US 3,862,106 AThermoplastic blend of partially cured monoolefin copolymer rubber and polyolefin plastic197557
US 3,970,722 AMethod for preparing a modified crystalline propylene polymer19769
US 4,087,485 APolypropylene blends having high impact strength and improved optical properties197895
US 4,087,486 APolypropylene composition containing EPR197833
US 4,105,718 APeroxide treated substantially amorphous polyolefin/hydrocarbon rubber blends useful as pressure-sensitive adhesives197823
US 4,140,732 AThermoplastic rubber compositions comprising polyolefin and sequential E/P or EPDM197915
US 4,143,099 AMethod of preparing a thermoplastic elastomeric blend of monoolefin copolymer rubber and polyolefin resin197943
JP S5524410 AMethod of manufacturing silicon semiconductor device—4
US RE30405 EThermoplastic blend of partially cured monoolefin copolymer rubber and polyolefin plastic198014
US 4,368,280 APartially cross-linkable compositions and process for preparing partially cross-linked thermoplastic elastomers198329
US RE31518 EDynamically partially cured thermoplastic blend of monoolefin copolymer rubber and polyolefin plastic198428