Abstract
Polypropylene composition having improved knit-line properties comprising from 5 to 30 parts by weight of a saturated ethylene-propylene rubber, correspondingly 95 to 70 parts by weight crystalline homopolymeric polypropylene and from 0.01 to 0.2 parts by weight of an organic peroxide per each 100 parts by weight of the total concentration of saturated ethylene-propylene rubber and polypropylene.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 33.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A polypropylene composition having improved knit-line properties comprising from 5 to 30 parts by weight of a saturated ethylene-propylene rubber, correspondingly 95 to 70 parts by weight crystalline homopolymeric polypropylene and from 0.01 to 0.2 parts by weight of an organic peroxide per each 100 parts by weight of the total concentration of saturated ethylene-propylene rubber and polypropylene.
- Claim 2Depends on #1
The composition of claim 1, wherein said ethylene-propylene rubber comprises from 75 to 30 percent by weight ethylene and correspondingly from 25 to 70 percent by weight propylene.
- Claim 3Depends on #1
The composition of claim 1, wherein said peroxide has a half-life of about 1 to 30 seconds at a temperature in the range of about 400° to 525° F.