Patents
US 4,143,099 A#1226189 Most CitedExpiredUnited States (USPTO)Utility

Method of preparing a thermoplastic elastomeric blend of monoolefin copolymer rubber and polyolefin resin

43Forward Citations (#1226189 Global)
0.9/yrCitation Velocity (#7822866 Global)
6.84Citation PageRank (#1989906 Global)
1Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of preparing a thermoplastic elastomeric blend comprising mixing from 90 to 10 parts by weight of monoolefin copolymer rubber with correspondingly from 10 to 90 parts by weight of polyolefin resin having tertiary hydrogen and a free radical generating curing agent therefor, masticating and shearing the mixture to produce a semi-cure of the rubber, completing the semi-cure before the onset of melting of the polyolefin resin, and ensuring that once the polyolefin has melted the level of free radicals remaining in the mixture is not sufficient to cause substantial degradation of the polyolefin.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 43.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a thermoplastic elastomeric blend comprising mixing from 75 to 10 parts by weight of monoolefin copolymer rubber with correspondingly from 25 to 90 parts by weight of polyolefin resin having tertiary hydrogen and a free radical generating peroxide curing agent therefor having a ten hour half-life temperature of from not less than 50° C. to less than 100° C., the amount of the active constituent of the curing agent in the blend not exceeding 1 part by weight per 100 parts of said rubber and resin together, masticating and shearing the mixture at an elevated temperature suf

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗