Coercivity in hot worked iron-neodymium boron type permanent magnets
Abstract
The coercivity of fine grain, hot worked RE2TM14B type permanent magnets is improved by quenching the material from a temperature greater than about 500 DEG C. to below about 100 DEG C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of increasing coercivity in a hot worked, rapidly solidified material consisting essentially of a predominant phase of hot work deformed fine grains of RE 2 TM 14 B and at least one coercivity contributing intergranular phase, said deformed fine grains contributing magnetic anisotropy to the hot worked material, said method comprising quenching the material to below 100° C. from an elevated temperature at which the equilibrium quantity of such intergranular phase is substantially greater than its equilibrium quantity below 100° C.
- Claim 2Independent Claim
A method of increasing coercivity in a hot worked, rapidly solidified material consisting essentially of a predominant phase of hot work deformed fine grains of RE 2 TM 14 B and at least one coerciv
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗