Permanent magnet containing rare earth metal, boron and iron
Abstract
A permanent magnet is obtained by pulverizing, molding and sintering a starting material containing an alloy ingot. The alloy ingot contains not less than 90% by volume of columnar crystals each having a columnar crystal grain size of 0.1 to 50 mu m along a short axis thereof and a columnar crystal grain size of larger than 100 mu m and not larger than 300 mu m along a long axis thereof, and is obtained by uniformly solidifying by a single roll method a molten alloy containing 25 to 31% by weight of a rare earth metal, 0.5 to 1.5% by weight of boron and iron under cooling conditions of a cooling rate of higher than 500 DEG C./sec. and not higher than 10,000 DEG C./sec. and a supercooling degree of 50 DEG to 500 DEG C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A permanent magnet obtained by pulverizing, molding and sintering a starting material comprising 70 to 99.9 vol. % of an alloy ingot, said alloy ingot containing not less than 90% by volume of columnar crystals each having a columnar crystal grain size of 0.1 to 50 μm along a short axis thereof and a columnar crystal grain size of larger than 100 μm and not larger than 300 μm along a long axis thereof, said alloy ingot having been obtained by uniformly solidifying by a single roll method a molten alloy containing 25 to 31% by weight of a rare earth metal, 0.5 to 1.5% by weight of boron and iro
- Claim 2Depends on #1
The permanent magnet as claimed in claim 1 wherein said rare earth metal is selected fr