Process for producing permanent magnets
Abstract
A process for producing permanent magnet materials, which comprises the steps of:forming an alloy powder having a mean particle size of 0.3-80 microns and composed of, in atomic percentage, 8-30 % R (provided that R is at least one of rare earth elements including Y), 2-28 % B, and the balance being Fe and inevitable impurities,sintering the formed body at a temperature of 900-1200°C,subjecting the sintered body to a primary heat treatment at a temperature of 750-1000°C,then cooling the resultant body to a temperature of no higher than 680°C at a cooling rate of 3-2000°C/min, andfurther subjecting the thus cooled body to a secondary heat treatment at a temperature of 480-700°C.35 MGOe, 40 MGOe or higher energy product can be obtained with specific compositions.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 17.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.