Patents
US 4,626,518 A#3552731 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing high toughness sintered bodies

22Forward Citations (#3552731 Global)
0.6/yrCitation Velocity (#14467745 Global)
9.64Citation PageRank (#1127709 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for manufacture of a high toughness sintered body, characterized by sintering a shaped body of a mixed powder consisting essentially of from 40 to 70% by weight of a first component of powdered ZrO 2 containing at least one stabilizer selected from the group consisting of Y 2 O 3 , CaO, and MgO and having an average particle diameter of not more than 1μ and from 30 to 60% by weight of a second component of powdered α-Al 2 O 3 having an average particle diameter of not more than 1 μm, which mixed powder may also contain not more than 3% by weight of SiO 2 , not more than 0.5% by weight of Fe 2 O 3 , or not more than 0.5% by weight of TiO 2 in a combined proportion of not more than 3% by weight at a temperature in the range of from 1400° C. to 1600° C. under normal pressure thereby producing a sintered body wherein at least 90% by weight of ZrO 2 particles present therein are accounted for by tetragonal and cubic crystals, the ratio of said tetragonal crystals to said cubic crystals is at least 1:3, and the average crystal particle diameter of the entire sintered body is at least 3μ.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacture of a high toughness sintered body, comprising: (a) preparing a powder mixture containing 40-99.5 wt% of Component A consisting essentially of ZrO 2 powder having an average particle diameter of no longer than 1 μm and 1-6 mol% of Y 2 O 3 , 7 mol% of MgO or 6 mol% of CaO as a stabilizer and 0.5-60 wt% of Component B consisting essentially of α-Al 2 O 3 powder having an average particle diameter of not longer than 1 μm by uniformally mixing water soluble salts of ZrO 2 , stabilizer and Al 2 O 3 in the form of an aqueous solution and coprecipitating the powder mixtu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Reed et al.; Ceramic Bulletin, vol. 55, p. 717 (1976).