Patents
US 4,659,529 A#26318084 Most CitedExpiredUnited States (USPTO)Utility

Method for the production of high strength polyacrylonitrile fiber

4Forward Citations (#26318084 Global)
0.1/yrCitation Velocity (#45375849 Global)
1.21Citation PageRank (#31481006 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Polyacrylonitrile (PAN) fiber of high strength (tensile strength≧20 g/d) produced from a polymer composed mainly of acrylonitrile (AN) and having a weight average molecular weight not less than 400,000, and a method of producing said fiber characterized by a multistage stretching step and a drying step under particular conditions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a high strength polyacrylonitrile fiber having a tensile strength not less than 20 g/d which comprises the following steps: (i) preparing a spinning solution of a polymer mainly composed of acrylonitrile, said polymer having a weight average molecular weight not less than 400,000, in which solution, the polymer molecular chains are sufficiently loosened or extended, and wherein the polymer is dissolved in an inorganic solvent under reduced pressure for defoaming so that the solution will not contain air bubbles; (ii) spinning the thus-obtained solution to form gel filam

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗