High-shrinkage acrylic fibers and the process for their production
Abstract
Acrylic yarns and fibers having a high shrinkage power, ranging up to 50%, obtained by wet spinning, a stretching of 1.3 to 3 × in air, washing, a stretching of 1 to 2.5 × into boiling water, drying, steaming at 105°-150° C., over-stretching of 1.2 to 2 × at 90°-100° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 5.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the production of acrylic yarns and fibers having a latent shrinkage of up to 50% in boiling water, characterized in wet spinning at least one solution of acrylic polymer, stretching the resulting filaments in air, at ambient temperature, in a ratio between 2 and 2.5×, washing with water, stretching in boiling water in a ratio between 1.05 and 1.8×, sizing, drying in the relaxed state in a zone kept at a dry temperature between 80° and 140° C. and a wet temperature between 50° and 70° C. for 1 to 30 minutes, steam treating in the relaxed state at a temperature between 105° and 15
- Claim 2Independent Claim
A process for the p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗