Patents
US 3,975,486 A#12758288 Most CitedExpiredUnited States (USPTO)Utility

Process for producing anti-pilling acrylic fiber

8Forward Citations (#12758288 Global)
0.2/yrCitation Velocity (#37875689 Global)
2.40Citation PageRank (#10866300 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a process for producing an anti-pilling acrylic fiber which has excellent level dyeing properties. This process involves dissolving an acrylonitrile in an inorganic solvent to prepare a spinning solution, wherein the inorganic solvent in the spinning solution is 40-70%, subjecting the spinning solution to wet-spinning by extrusion through spinneret orifices into a coagulation bath containing an inorganic solvent in an amount of 50-70% of that in the spinning solution, while maintaining the linear velocity ratio of free extrusion at 1 or higher and the jet stretch ratio 1.5 or higher, stretching the formed gel fibers 3-7 times the length in hot water or in a heated steam medium at 80°-120°C, drying the stretched fibers and then subjecting the fibers to a relaxation treatment in a hot air current at a temperature of 150°C or lower or in a wet heat atmosphere at a temperature of 120°C or lower. The jet stretch ratio is defined as being the quotient obtained by dividing the takeup speed of the coagulated filaments from the coagulation step by the linear velocity of extrusion of the spinning solution through the spinneret orifices.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing an anti-pilling acrylic fiber which comprises dissolving an acrylonitrile polymer in a rhodanide solvent to prepare a spinning solution, wherein a rhodanide solvent in the spinning solution is 40-70%, subjecting the spinning solution to wet-spinning by extrusion through spinneret orifices into a coagulation bath containing a rhodanide solvent in an amount of 50-70% of that in the spinning solution, while maintaining the linear velocity ratio of free extrusion at 1 or higher, and the jet stretch ratio 1.5 or higher, stretching the formed gel fibers 3-7 times the length i

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗