Polyether esters for the cementing of textiles
Abstract
A polyether ester having a melting point of 95 DEG to 125 DEG C. based on 1,4-butanediol, terephthalic acid and isophthalic acid in a molar ratio of 48 to 55:52 to 45 and a content of 10.5 to 25 wt % of polyethylene glycol with a molar mass of 0.4 to 6 kg/mol is presented as a suitable fusion adhesive for textiles. The bonds prove to be resistant to hot water and perchloroethylene.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Polyether ester for the cementing of textiles comprising terephthalic acid, isophthalic acid, 1,4-butanediol and a polyalkylene ether diol, having a melting point of 95° to 125° C. and a relative viscosity, measured at 25° C. on 1 g of polyether ester in 100 ml of a mixture of 60-wt-parts of phenol and 40 wt-parts of 1,1,2,2,-tetrachloroethane, from 1.85 to 2.20, wherein the molar ratio of terephthalic acid to isophthalic acid is 48 to 55:52 to 45 having a content of 10.5 to 25 wt % of polyalkylene ether diol with a molar mass of 0.4 to 6 kg/mol, relative to the weight sum of all the residues
- Claim 2Depends on #1
Polyether ester as claimed in claim 1, wherein said polyalkylene ether diol is polyethylene glycol.
- Claim 3Depends on #1
Polyether ester as claimed in claim 1, wherein said molar ratio of terephthalic aci
Technical Overview & Description