Thermoplastic copolyesters, processes for their preparation and their use
Abstract
Thermoplastic copolyesters which have a minimum relative viscosity of 1.7 and contain (a) 35-47.5 mol % of units of terephthalic acid, (b) 15-2.5 mol % of units of isophthalic acid, (c) 10-30 mol % of units of ethylene glycol and (d) 40-20 mol % of units of diethylene glycol, it being possible for up to 9 mol % of the units of ethylene glycol to be replaced by units of a bisphenol dihydroxyalkyl ether, are very suitable as hot-melt adhesives.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A thermoplastic copolyester which has a minimum relative viscosity of 1.7, measured at 30° C. on a solution of 1 g of polyester in 100 ml of a solvent consisting of equal parts of phenol and symmetrical tetrachloroethane, and contains condensed units of a mixture of aromatic dicarboxylic acids and also of aliphatic diols, and which contains, based on the polyester, (a) 35-47.5 mol % of units of terephthalic acid, (b) 15-2.5 mol % of units of isophthalic acid, (c) 10-30 mol % of units of ethylene glycol and (d) 40-20 mol % of units of diethylene glycol, it being possible for up to 9 mol % of th
- Claim 2Depends on #1
A copolyester according to claim 1, which has a relative viscosity of 1.7 to 4.0.
- Claim 3Depends on #1
A copolyester according to claim 1, which conta
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗