In mfr. of polyarylesters of iso- and/or tere-phthalic acids, to a degree of condensn. corresp. to a melt viscosity >80,000 P at 300 degrees C, by condensn. of a precondensate of melt viscosity >2,000 P at 270 degrees C, the precondensate is introduced into a twin-screw…
Schade Gerhard
A water-dispersible polycondensation polyester resin having moieties of at least one polycarboxylic acid and at least one polyvalent alcohol having a terminal hydroxyl group, said polyester having a molecular weight between 300 and 3,000, a softening point between 30° and 60° C,…
A method for the preparation of mixed polyesters with the use of titanium catalysts, wherein addition products prepared from phosphorous acid and monoepoxides are utilized, especially in the esterification stage and the subsequent polycondensation stage of the process. The…
Thermosetting coating substances containing as binding agent 5 to 35 weight-percent of triazine resins, especially benzoguanamine resins, or blocked polyisocyanate resins, and 95 to 65 weight-parts of saturated polyesters of terephthalic and/or isophthalic acids and 100 to 70…
A process for preparing a poly-(alkylpentamethyleneterephthalamide) which comprises heating an aqueous solution of the corresponding nylon salt and still water soluble low molecular weight oligomer, the mixture of nylon salt and oligomer having 20 to 50 mole percent carbonamide…
TRANSPARENT POLYAMIDES RESISTANT TO BOILING ARE PRODUCED BY REACTING AN AROMATIC DICARBOXYLIC ACID (OR AN AMIDE-FORMING DERIVATIVE THEREOF) WITH A DIAMINE HAVING THE GENERAL FORMULA: H2N-CH(-R1)-R2-CH(-R3)-NH2 WHEREIN R1 IS HYDROGEN OR AN ALKYL GROUP OF 1 TO 4 CARBON ATOMS, R2…
A process for producing a linear polyester which comprises: (1) condensing excess 1,4-butanediol with a lower alkyl ester of an aromatic dicarboxylic acid at a temperature of less than 200° C; (2) removing uncondensed 1,4-butanediol therefrom so that the reaction mixture…
A polymeric formal having the general formula ##STR1## wherein p is 0 or 1, n is a positive integer from 2 to 200 and R represents optionally halogen-substituted straight-chained or branched-chained alkyl radicals having 3 to 8 carbon atoms, an aryl radical or an aralkyl radical…
Poly-(arylene-triketoimidazolidines) are prepared by reacting approximately diamine amounts of bis- (oxalic acid-monoalkyl ester-monoamide) of an aromatic diamine with an aromatic diisocyanate in a polar organic solvent at an elevated temperature. The polymers melt at about 310*…
A polyamide composition, useful in the preparation of transparent sheets, having improved resistivity toward solvents containing moieties of terephthalic acid and 2-methylpentamethylenediamine, said polyamide characterized by a content of moieties of 2-ethyltetramethyldiamine…
A polyether ester having a melting point of 95 DEG to 125 DEG C. based on 1,4-butanediol, terephthalic acid and isophthalic acid in a molar ratio of 48 to 55:52 to 45 and a content of 10.5 to 25 wt % of polyethylene glycol with a molar mass of 0.4 to 6 kg/mol is presented as a…
1. Claim (for the Contracting States : BE, CH, DE, FR, GB, IT, LI, LU, NL, SE) Polyamides obtained by polycondensation of a mixture of a) 10-50 mol % decanedicarboxylic acid, b) 10-80 mol % 5-tert-butyl-isophthalic acid c) 0-70 mol % isophthalic acid and/or terephthalic acid and…
L'invention concerne un procédé de préparation de poly-(alkylpentaméthylènetéréphtalamide) éventuellement modifié. On chauffe des solutions aqueuses des sels de nylon correspondants mélangés avec des oligoamides à bas poids moléculaire, encore solubles dans l'eau, avec…
A process for the manufacture of wire insulation varnish resins suitable for application from the melted state which comprises: 1. Contacting a lower alkyl ester of terephthalic acid with tris-(hydroxyethyl)-isocyanurate and ethylene glycol in the presence of a trans…
A polyether ester having a melting point of 95 DEG to 125 DEG C. based on 1,4-butanediol, terephthalic acid and isophthalic acid in a molar ratio of 48 to 55:52 to 45 and a content of 10.5 to 25 wt % of polyethylene glycol with a molar mass of 0.4 to 6 kg/mol is presented as a…
PROCESS OF PRODUCING ESTER RESIN CONTAINING ISOCYANURATE GROUPS AND IMIDE GROUPS IN THE POLYMER CHAIN COMPRISING CONDENSING A POLYALCOHOL WITH A TRICARBOXYLIC ACID OF THE FORMULA: 1,3,5-TRI(R-),2,4,6-TRI(O=)HEXAHYDRO-S-TRIAZINE WHEREIN R REPRESENTS A MOIETY HAVING THE FORMULA:…
1. Claims for the Contracting States : BE, CH, DE, FR, GB, IT, LI, LU, NL, SE Polyamides obtained by polycondensing a mixtures of a) 20-65 mol-% of isophthalic acid b) 35-60 mol-% of decanedicarboxylic acid c) 0-30 mol-% of tert. butylisophthalic acid as well as d) 50-100 mol-%…
A process for producing unsaturated polyester resins from conventionally employed unsaturated and optionally saturated dicarboxylic acids and polyhydric alcohols wherein the esterification catalyst employed is an alkali tetraphenylborate or a zirconate of 2-alkyl-1,3-hexanediol…