Abstract
THE INVENTION RELATES TO A PROCESS FOR ANNEALING STEEL POWDER. THE POWDER IS CONTINUOUSLY PASSED THROUGH AN ANNEALING FURNACE AND HEATED TO A TEMPERATURE IN THE RANGE OF 1450*F. TO 2100*F. WHILE EXPOSED TO A REDUCING GAS. THE DEW POINT OF THE FURNACE ATMOSPHERE IS MAINTAINED AT A VALUE SLIGHTLY BELOW THE EQUILIBRIUM VALUE THROUGHOUT THE LENGTH OF THE HEATING ZONE BY ADJUSTMENT OF THE RATE OF FLOW OF THE REDUCING GAS TO THE FURNACE. BY MAINTAINING THE DEW POINT OF THE FURNACE ATMOSPHERE WITHIN PRECISE LIMITS, A SUBSTANTIALLY COMPLETE REDUCTION OF THE CARBON CONTENT OF THE STEEL PARTICLES IS OBTAINED AND WELDING OF THE PARTICLES IS PREVENTED, SO THAT THE SINTERED CAKE OF PARTICLES CAN BE READILY BROKEN UP AFTER ANNEALING TO RESTORE THE AS-ATOMIZED PARTICLE SIZE AND THEREBY PROVIDE AN INCREASE DENSITY FOR THE COMPACTED AND SINTERED PART.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.