Abstract
A method for producing a low carbon ferrous powder melt stock with a sulfur content of less than 5 parts per million is disclosed comprising the steps of atomizing molten steel into a powder, exposing the powder to a temperature of at least 2100° F. in a hydrogen containing atmosphere until the sulfur content has been reduced to the desired level, and cooling the desulfurized powder to ambient temperature in a non-oxidizing atmosphere. During heat treatment an interconnected porosity of at least 10% is maintained for the powder.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of preparing ferrous powder melt stock containing a maximum of about 5 parts per million sulfur, comprising the steps of: a. forming a molten ferrous alloy into a powder having sulfur in reducible form and having an average particle size of less than about 0.09 inch, b. while maintaining an interconnected porosity of at least 10% for the powder, exposing the powder to a temperature of at least 2100° F. in a hydrogen containing atmosphere from a time of at least about 1 hour until the sulfur content of the powder is reduced to less than or equal to about 5 parts per million to form a
- Claim 2Depends on #1
A method as set forth in claim 1 wherein the powder, before desulfurizing, contains 45 to 170 ppm sulfur.
- Claim 3Independent Claim
A metho
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (1)
- The Metal--Iron, Alloys of Iron Monographs by Cleaves and Thompson p. 69 (1935).