Iron powder of high compressibility and low bulk density is made by atomizing a stream of molten steel by means of a conical jet of water at a rate in excess of 10 cubic meters water per metric ton of steel, the half cone angle is between 40° and 60°, preferably 45°; and air suction is provided in a region upstream from the cone, adjacent to the stream at a pressure of 0.02 to 0.20 bars below ambient, by means of a length adjustable tube extending down from the nozzle chamber. The powder is reduced at 1,000° C. to 1,200° C., and the resulting cake is broken up to obtain a powder having a particle size distribution with a higher content of larger particles than the powder immediately resulting from the atomization.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 9.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Method of making an iron powder of high compressibility and low bulk density by means of atomizing a stream of molten steel, comprising the steps of: providing a conical jet of water at a water pressure prior to jet formation in excess of 80 bars and at a rate in excess of 10 cubic meters water per metric ton of steel, the cone of the jet having an angle so that the water impinges upon the stream at an angle between 40° and 60°; providing air suction in a region upstream from the cone, adjacent to the stream at a pressure of 0.02 to 0.20 bars below ambient; annealing the powder in a reduci

  2. Claim 2Independent Claim