Patents
US 11,236,016 B2#44972595 Most CitedActiveUnited States (USPTO)Utility

Chemically strengthened glass

2Forward Citations (#44972595 Global)
0.5/yrCitation Velocity (#16886802 Global)
0.88Citation PageRank (#49009329 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The purpose of the present invention is to provide a chemically strengthened glass in which reduction in glass surface strength is effectively suppressed even without performing a polishing treatment after a prolonged chemical strengthening treatment has been conducted at a high temperature. The present invention relates to a chemically strengthened glass having a specific glass composition, wherein: the surface roughness (Ra) is a specific value or greater; the compressive stress layer depth of a surface layer is a specific value or greater; by setting the hydrogen concentration in the glass surface layer to be within a specific range, the surface strength of the glass is dramatically improved even without performing an etching treatment using hydrofluoric acid or polishing the glass surface after a prolonged chemical strengthening treatment has been conducted at a high temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A chemically strengthened glass comprising a compressive stress layer that is formed in a surface layer of the glass by an ion exchange method, wherein: the glass has a surface roughness (Ra) of 0.50 nm or more; the glass has a depth of the compressive stress layer of 55 μm or more; the glass has a composition comprising, in mole percentage on an oxide basis, 55.5 to 76.5% of SiO 2 , 5 to 20% of Al 2 O 3 , 8 to 25% of Na 2 O and 0.1% or more of P 2 O 5 ; a hydrogen concentration Y1 in a region of a depth X from an outermost surface of the chemically strengthened glass satisfies Expression (I)

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

Non-Patent Literature (5)

  • International Search Report dated Jul. 17, 2018 in PCT/JP2018/016503, filed on Apr. 23, 2018 (with English translation).
  • S. Ilievski et al., “Practical IR extinction coefficients for water in commercial glasses determined by nuclear reaction analysis”, Glastech. Ber. Glass Sci. Technol., 73 (2000) pp. 39-45.
  • S. Ito et al., “Crack Blunting of High-Silica Glass”, Journal of the American Ceramic Society, vol. 65, No. 8,(1982), pp. 368-371.
  • Won-Taek Han et al., “Effect of residual water in silica glass on static fatigue”, Journal of Non-Crystalline Solids, 127, (1991) pp. 97-104.
  • Written Opinion dated Jul. 17, 2018 in PCT/JP2018/016503, filed on Apr. 23, 2018.