Strengthened glass articles having improved survivability
Abstract
Embodiments are directed to strengthened glass articles comprising a thickness t≤1 mm (1000 μm), an inner region under a central tension CT (in MPa), and at least one compressive stress layer adjacent the inner region and extending within the strengthened glass article from a surface of the strengthened glass article to a depth of layer DOL (in μm), wherein the strengthened glass article is under a compressive stress at the surface CSs (in MPa), wherein the strengthened glass article is an alkali aluminosilicate glass article comprising 0-5 mol % Li2O, and at least 3 mol % Al2O3, and wherein the DOL≥70 μm, and a CSs/DOL ratio≥2.5 MPa/μm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A strengthened glass article comprising: a thickness t≤1 mm, an inner region under a central tension CT, and at least one compressive stress layer adjacent the inner region and extending within the strengthened glass article from a surface of the strengthened glass article to a depth of layer DOL, wherein the DOL is greater than or equal to 70 μm, wherein the strengthened glass article is under a compressive stress at the surface CSs, wherein the strengthened glass article is an alkali aluminosilicate glass article comprising 0 mol % Li2O, and at least 3 mol % Al2O3, and wherein the strengthen
- Claim 2Independent Claim
The strengthened glass articl