Patents
US 10,150,698 B2#16154135 Most CitedActiveUnited States (USPTO)Utility

Strengthened glass with ultra deep depth of compression

7Forward Citations (#16154135 Global)
0.9/yrCitation Velocity (#8297732 Global)
1.26Citation PageRank (#29705136 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A glass article, the glass article comprising a thickness t and a compressive region having a compressive stress CS s in a range from about 400 MPa to about 1200 MPa at a surface of the glass article, wherein the compressive region extends from the surface to a depth of compression DOC, wherein 0.1·t≤DOC≤0.25·t, and has a compressive stress profile, the compressive stress profile comprising: a. a first portion b extending from the surface to a depth d b below the surface and having a slope m b , wherein −40 MPa/μm≥m b ≥−200 MPa/μm; and b. a second portion c extending from about d c to the d

  2. Claim 2Depends on #1

    The glass article of claim 1 , wherein the depth of compression DOC is in a range from about 95 μm to about 250 μm.

  3. Claim 3Independent Claim

    Th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,433,611 AStrengthening glass by multiple alkali ion exchange1969228
GB 1,334,828 ASoda-silica glass—70
US 3,798,013 ADouble ion exchange method for strengthening glass articles1974232
US 3,936,287 AMethod for making glass-ceramic articles exhibiting high frangibility197668
US 4,042,405 AHigh strength ophthalmic lens197793
US 4,726,981 AStrengthened glass articles and method for making198861
US 5,350,607 AIonized cluster beam deposition of sapphire199425
EP 0,700,879 A1Scratch-resistant aluminium oxide coating on a glass substrate and process for its manufacture—17
US 5,773,148 AChemically toughened pane199867
US 5,895,768 AChemically prestressable aluminosilicate glass and products made therefrom199986
US 6,111,821 ATransparent and scratchproof watch crystal and watch case fitted with such a crystal200016
WO 2005/091021 A1Scratch-resistant optical multi-layer system applied to a crystalline substrate—12
US 2005250639 A1Lithium-aluminosilicate flat float glass—138
US 2007060465 A1Chemically strengthened lithium aluminosilicate glass having high strength effective to resist fracture upon flexing from impact of high velocity projectiles—88
JP 2009099239 AProcess for producing glass substrate for magnetic disk and magnetic disk—36
US 2009197088 A1Tempered glass substrate and method of producing the same—170
US 2010003508 A1Optical article with antistatic and antiabrasive properties, and method for producing same—36
WO 2010/005578 A1Glass with compressive surface for consumer applications—44
US 2010028607 A1Dual stage ion exchange for chemical strengthening of glass—111
US 2010035038 A1Strengthened glass articles and methods of making—194
US 2010087307 A1Strengthened glass substrate and process for producing the same—97
US 2010119846 A1Reinforced plate glass and method for manufacturing the same—114
JP 2010202514 AGlass substrate for mobile liquid crystal display and method for producing the same, and mobile liquid crystal display using the same—23

Non-Patent Literature (5)

  • Aegerter et al; "Sol-gel technologies for glass producers and users-Chapter 4.1.8-Scratch resistant coatings (G. Helsch and G. H. Frischat)", pp. 217-221, Kluwer Academic Publishers, 2004.
  • Aegerter et al; “Sol-gel technologies for glass producers and users—Chapter 4.1.8—Scratch resistant coatings (G. Helsch and G. H. Frischat)”, pp. 217-221, Kluwer Academic Publishers, 2004.
  • ASTM C1279-13 "Standard Test Method for Non-Destructive Photoelastic Measurement of Edge and Surface Stresses in Annealed, Heat-Strengthened, and Fully Tempered Flat Glass".
  • ASTM C1422/C1422M-10 "Standard Specification for Chemically Strengthened Flat Glass".
  • ASTM C1422/C1422M—10 “Standard Specification for Chemically Strengthened Flat Glass”.