Patents
US 6,136,099 A#6710513 Most CitedExpiredUnited States (USPTO)Utility

Rare earth-iron series permanent magnets and method of preparation

14Forward Citations (#6710513 Global)
0.5/yrCitation Velocity (#14700645 Global)
3.43Citation PageRank (#6110140 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A rare earth-iron series magnet formed from an alloy ingot using a one-step hot working process is provided. The alloy ingot includes between about 8 and 30 atomic percent of at least one rare earth element, between about 2 and 28 atomic percent of boron, less than about 50 atomic percent of cobalt, less than about 15 atomic percent of aluminum and the balance of iron and other impurities that are inevitably included during the preparation process. The alloy is cast to obtain a cast ingot and the hot working is performed on the cast ingot at a temperature of greater than about 500 DEG C. in order to make the crystal grains of the ingot fine and to align the axis of the grains in a desired direction.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a permanent magnet having as principal constituents at least one rare earth metal, iron, boron and copper, comprising: providing a magnet alloy composition including at least one rare earth metal, iron, boron and copper; melting the magnet alloy composition including the rare earth metal, iron, boron and copper, casting the alloy composition into an ingot, hot working the alloy ingot at a temperature of at least about 500° C. with a strain rate of from about 10 -4 to 10 2 per second.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the strain rate is from about 10 -4 to 1 per second.

  3. Claim 3Depends on #1

    The method of claim 1, further including the step of heat-treating the cast alloy ingot at a temperature of at least 250° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Cedighian, "Die magnetischen Werkstoffe", VDI Verlag, Dusseldorf, pp. 28-35, 1973.
  • Cedighian, Die magnetischen Werkstoffe , VDI Verlag, Dusseldorf, pp. 28 35, 1973.
  • Chemical Abstracts, Kononenko, et al., "Effect of Heat Treatment on the Coercive Force of Neodymium-Iron-Boron Alloy Magnets", vol. 104, No. 24, p. 705, Jun. 1986.
  • Chemical Abstracts, Kononenko, et al., Effect of Heat Treatment on the Coercive Force of Neodymium Iron Boron Alloy Magnets , vol. 104, No. 24, p. 705, Jun. 1986.
  • Chin, "(FeCo)-Nd-B Permanent Magnets By Liquid Dynamic Compaction", J. Appl. Phys. 59(4), Feb. 15, 1986, pp. 1297-1300.