According to the process, a heap preferably having dimensions of at least 2.5 m high and 5 m wide is constructed with chalcopyrite bearing ore. The constructed heap includes exposed sulfide mineral particles at least 25 weight % of which are chalcopyrite. The concentration of…
Shrader Vandy
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap of refractory sulfide ore particles with a…
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap of refractory sulfide ore particles with a…
According to the process, a heap preferably having dimensions of at least 2.5 m high and 5 m wide is constructed with hypogenic copper sulfide bearing ore. The constructed heap includes exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper…
A heap (20) is constructed with chalcopyrite bearing ore. The constructed heap (20) includes exposed sulfide mineral particles wherein at least 25 weight percent of which are chalcopyrite. The concentration of the exposed sulfide mineral particles in the heap (20) is such that…
According to the process, a heap preferably having dimensions of at least 2.5 m high and 5 m wide is constructed with hypogenic copper sulfide bearing ore. The constructed heap includes exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap of refractory sulfide ore particles with a…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap (10) of refractory sulfide ore particles with…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap (10) of refractory sulfide ore particles with…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A heap is constructed with hypogenic copper sulfide bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are hypogenic copper sulfides. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of…
A heap is constructed with chalcopyrite bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are chalcopyrite. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of exposed sulfide sulfur per…
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap (10) of refractory sulfide ore particles with…
A heap (20) is constructed with chalcopyrite bearing ore. The constructed heap (20) includes exposed sulfide mineral particles wherein at least 25 weight percent of which are chalcopyrite. The concentration of the exposed sulfide mineral particles in the heap (20) is such that…
A heap (20) is constructed with chalcopyrite bearing ore. The constructed he ap (20) includes exposed sulfide mineral particles wherein at least 25 weight percent of which are chalcopyrite. The concentration of t he exposed sulfide mineral particles in the heap (20) is such that…