A high temperature heap bioleaching process for extracting copper.
Abstract
A heap is constructed with chalcopyrite bearing ore to include exposed sulfide mineral particles at least 25 weight % of which are chalcopyrite. The concentration of the exposed sulfide mineral particles is such that the heap includes at least 10 Kg of exposed sulfide sulfur per tonne of solids in the heap. At least 50% of the total copper in the heap is in the form of chalcopyrite. A substantial portion of the heap is heated to at least 50° C. The heap is inoculated with a thermophilic microorganism, and bioleaching is carried out so that sufficient sulfide mineral particles in the heap are biooxidized to oxidize at least 10 Kg of sulfide sulfur per tonne of solids in the heap and to cause the dissolution of at least 50% of the copper in the heap in a relatively short period of time.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,766,930 A | Method of biotreatment for solid materials in a nonstirred surface bioreactor | 1998 | 37 |