Patents
Inventor / Author Profile

Schoen J

7Total Forward Citations
8Indexed Patents
1Patent H-Index
US 3,737,343 A#16228220 Most Cited · 6 citations0.1/yr · PR 7.26ExpiredUS · Utility
Technique for the preparation of ion implanted tantalum-aluminum alloy
Inventors: Basseches H, Gerstenberg D, Lepselter M, Macrae A, Schoen JAssignee: Bell Telephone Labor IncFiled 1971-04-19 · Granted 1973-06-05

A TECHNIQUE FOR THE PREPARATION OF TANTALUM-ALUMINUM ALLOY FILMS MANIFESTING RESISTIVITIES WITHIN THE RANGE OF 10-**3 TO 10-**2 OHM-CENTIMETERS WHICH ARE STABLE AT TEMPERATURES OF THE ORDER OF 400*C. INVOLVES DEPOSITING TANTALUM-ALUMINUM ALLOY FILMS BY CONVENTIONAL CONDENSATION…

CN 1,077,601 C#108351578 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
Method for producing silicon-chromium grain oriented electrical steel
Inventors: Schoen J W, Dahlstrom N A, Klapheke C GAssignee: Armco IncFiled 1997-11-28 · Granted 2002-01-09

The present invention provides a method of producing grain oriented electrical steels. A hot processed strip consisting essentially of 2.5-4.5% silicon, 0.1-1.2% chromium, less than 0.050% carbon, less than 0.005% aluminum, up to 0.1% sulfur, up to 0.14% selenium, 0.01-1%…

CN 119,136,829 A#65748984 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
SARS-CoV-2 virus attenuated by one to stop

The present invention relates to polynucleotides encoding attenuated SARS-CoV-2 or fragments thereof, wherein the polynucleotides comprise at least 20to terminal codons. The polynucleotide may comprise further modifications and may be comprised in attenuated SARS-CoV-2. The…

YU 46,929 B#81520155 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredYU · Utility
Postupak ultrabrze termičke obrade elektro čelika sa orijenisanom strukturom
Inventors: Schoen J W, Margerum D EAssignee: Armco Advanced MaterialsFiled 1989-03-24

Ultra-rapid annealing of grain oriented electrical steel to a temperature prior to the final high temperature anneal results in improved texture and smaller secondary grain size. The ultra-rapid anneal requires heating the strip to a temperature above about 677 DEG C (1250 DEG…

YU 46,930 B#143213830 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredYU · Utility
Postupak za izradu trake neorijentisanog elektro čelika
Inventors: Schoen J WAssignee: Armco Advanced MaterialsFiled 1989-03-24

POSTUPAK ZA IZRADU TRAKE NEORIJENTISANOG ELEKTRO ČELIKA, koji ima veliku gustinu magnetnog fluksa, naznačen time, što se čelik ultra-brzo odgreva brzinom od preko 100В°C u sekundi, do temperature od 750 do 1150В°C, za period kvašenja manji od pet minuta. Prijava sadrži 10…