Ultra-rapid annealing of grain oriented electrical steel to a temperature prior to the final high temperature anneal results in improved texture and smaller secondary grain size. The ultra-rapid anneal requires heating the strip to a temperature above about 677 DEG C (1250 DEG…
Inventor / Author Profile
Margerum D E
0Total Forward Citations
1Indexed Patents
0Patent H-Index
Frequent Co-Inventors: Schoen J W