EP 1,637,271 B1#6999332 Most Cited · 14 citations0.9/yr · PR 2.31ExpiredEP · Utility
Process for diffusion welding with low deformation of sintered nonoxidised ceramic components
Inventors: Meschke Frank Dr, Kayser Ursula, Rendtel Andreas DrAssignee: Esk Ceramics Gmbh & Co KgFiled 2005-09-06 · Granted 2011-05-18

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

EP 1,637,271 A1#8682195 Most Cited · 12 citations0.6/yr · PR 1.67PendingEP · Application
Process for diffusion welding with low deformation of sintered nonoxidised ceramic components ; Article made of a no oxide ceramic with a seam free connection

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

EP 3,339,658 A1#9521451 Most Cited · 11 citations1.4/yr · PR 1.94PendingEP · Application
Connecting element for the friction-increasing connection of components, process for making a connecting element and use of a connecting element

The present disclosure relates to a connecting element and to a process for producing said connecting element. The present disclosure further relates to the use of said connecting element for friction-increasing connection of components to be joined in machine, plant and motor…

US 2009239007 A1#12206257 Most Cited · 9 citations0.5/yr · PR 1.55PendingUS · Application
Process for the low-deformation diffusion welding of ceramic components

A process for joining ceramic components, wherein the components which are to be joined consist of sintered nonoxide ceramic, and the components are brought into contact with one another in a diffusion-welding process in the presence of a shielding gas atmosphere and are joined…

US 2007235122 A1#13077794 Most Cited · 8 citations0.4/yr · PR 2.05PendingUS · Application
Process for the low-deformation diffusion welding of ceramic components

A process for joining ceramic components, wherein the components which are to be joined consist of sintered nonoxide ceramic, and the components are brought into contact with one another in a diffusion-welding process in the presence of a shielding gas atmosphere and are joined…

DE 102004044942 A1#17155277 Most Cited · 6 citations0.3/yr · PR 1.84PendingDE · Application
Verfahren zum verformungsarmen Diffusionsschweißen von keramischen Komponenten

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

KR 20070043884 A#22426230 Most Cited · 5 citations0.3/yr · PR 1.12ExpiredKR · Utility
Process for the low-deformation diffusion welding of ceramic components

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

JP 2006083057 A#24725976 Most Cited · 4 citations0.2/yr · PR 1.39ExpiredJP · Utility
Method for low-deformation diffusion-welding of ceramic component

<P>PROBLEM TO BE SOLVED: To provide a method for joining ceramic components consisting of sintered non-oxide ceramics to each other to form a seamless monolith. <P>SOLUTION: In the method for joining the ceramic components, the components to be joined consist of the…

US 2019323529 A1#25190215 Most Cited · 4 citations0.6/yr · PR 1.33PendingUS · Application
Connecting element for the friction-increasing connection of components, process for making a connecting element and use of a connecting element

The present disclosure relates to a connecting element and to a process for producing said connecting element. The present disclosure further relates to the use of said connecting element for friction-increasing connection of components to be joined in machine, plant and motor…

CN 110,114,584 A#29763091 Most Cited · 3 citations0.4/yr · PR 1.28ActiveCN · Utility
Friction for component increases the connecting element of connection, is used to prepare the method for connecting element and the purposes of connecting element

This disclosure relates to a kind of connecting element and the method for being used to prepare the connecting element.Present disclosure also relates to the purposes of the connecting element, increase connection for the friction of component to be joined in machine, equipment…

DD 291,490 A5#43177203 Most Cited · 2 citations0.1/yr · PR 0.94ExpiredDD · Utility
Pressform zur herstellung von matrizen aus keramik

Die Erfindung betrifft das Gebiet der Metallformung und ist zur Herstellung von Formgebungswerkzeugen auf der Basis von Matrizen aus Keramik fuer die Formgebung von Metallen durch Ziehen, Stoszen, Druecken oder Extrudieren anwendbar. Erfindungsgemaesz ist in einem…

EP 3,663,436 A1#41000890 Most Cited · 2 citations0.3/yr · PR 0.99PendingEP · Application
Connecting element for the friction-increasing connection of components, process for making a connecting element and use of a connecting element
Inventors: Grimm Florian, Rendtel AndreasAssignee: 3m Innovative Properties CoFiled 2018-12-05

The present disclosure relates to a connecting element and to a process for producing said connecting element. The present disclosure further relates to the use of said connecting element for friction-increasing connection of components to be joined in machine, plant and motor…

US 11,015,625 B2#44131164 Most Cited · 2 citations0.4/yr · PR 0.91ActiveUS · Utility
Connecting element for the friction-increasing connection of components, process for making a connecting element and use of a connecting element

The present disclosure relates to a connecting element and to a process for producing said connecting element. The present disclosure further relates to the use of said connecting element for friction-increasing connection of components to be joined in machine, plant and motor…

US 8,087,567 B2#45318503 Most Cited · 2 citations0.1/yr · PR 0.87ActiveUS · Utility
Process for the low-deformation diffusion welding of ceramic components
Inventors: Meschke Frank, Kayser Ursula, Rendtel AndreasAssignee: Meschke Frank, Kayser UrsulaFiled 2009-04-14 · Granted 2012-01-03

A process for joining ceramic components, wherein the components which are to be joined consist of sintered nonoxide ceramic, and the components are brought into contact with one another in a diffusion-welding process in the presence of a shielding gas atmosphere and are joined…

WO 2006/029741 A1#39681115 Most Cited · 2 citations0.1/yr · PR 1.02PendingWO · Application
Method for the low-deformation diffusion-welding of sintered unoxidised ceramic components, and structure consisting of unoxidised ceramic with a seamless join

The invention relates to a method for joining ceramic components, said method being characterised in that the components to be joined consist of sintered unoxidised ceramic. The components are brought into contact by means of a diffusion-welding method in the presence of a…

RU 2,353,486 C2#49916340 Most Cited · 1 citations0.1/yr · PR 0.87ExpiredRU · Utility
Method of low-deforming diffusion welding of elements made from sintered non-oxide ceramics and workpiece made from non-oxide ceramics with seamless joint
Inventors: Meshke Frank, Kajzer Ursula, Rendtel AndreasAssignee: Ehsk Keramiks Gmbkh Und Ko KgFiled 2005-09-06 · Granted 2009-04-27

FIELD: welding jobs. SUBSTANCE: invention can be used for jointing ceramic elements made from sintered non-oxide ceramics. The elements are brought in contact and jointed by diffusion welding in a low-deforming way, in the presence of protective gas and with a forced applied to…

WO 2018/118899 A1#60597010 Most Cited · 1 citations0.1/yr · PR 0.76PendingWO · Application
Connecting element for the friction-increasing connection of components, process for making a connecting element and use of a connecting element

The present disclosure relates to a connecting element and to a process for producing said connecting element. The present disclosure further relates to the use of said connecting element for friction-increasing connection of components to be joined in machine, plant and motor…

CA 2,579,347 A1#69484481 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Process for the low-deformation diffusion welding of ceramic components

The invention relates to a method for joining ceramic components, said method being characterised in that the components to be joined consist of sintered unoxidised ceramic. The components are brought into contact by means of a diffusion-welding method in the presence of a…

CA 2,579,347 C#74469194 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Process for the low-deformation diffusion welding of ceramic components
Inventors: Meschke Frank, Kayser Ursula, Rendtel AndreasAssignee: Esk Ceramics Gmbh & Co KgFiled 2005-09-06 · Granted 2013-06-18

A process for joining ceramic components, wherein the components which are to be joined consist of sintered nonoxide ceramic, and the components are brought into contact with one another in a diffusion-welding process in the presence of a shielding gas atmosphere and are joined…

ES 2,362,190 T3#144325900 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Procedimiento para el soldeo por difusión con poca deformación de componentes cerámicos sinterizados no oxídicos.
Inventors: Meschke Frank, Kayser Ursula, Rendtel AndreasAssignee: Esk Ceramics Gmbh & Co KgFiled 2005-09-06 · Granted 2011-06-29

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

HK 1,091,165 A1#133866084 Most Cited · 0 citations0.0/yr · PR 0.56PendingHK · Application
A process for joining ceramic components and monoliths produced thereof

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…

KR 20190095401 A#62555753 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
구성요소들의 마찰-증가 연결을 위한 연결 요소, 연결 요소를 제조하기 위한 방법, 및 연결 요소의 용도

본 발명은 연결 요소, 및 상기 연결 요소를 제조하기 위한 방법에 관한 것이다. 본 발명은 또한 기계, 플랜트 및 자동차 구성 및 에너지 생성에서 결합될 구성요소들의 마찰 증가 연결을 위한 상기 연결 요소의 용도에 관한 것이다.

NO 20,071,913 L#72898654 Most Cited · 0 citations0.0/yr · PR 0.56ActiveNO · Utility
Fremgangsmate for lavdeformasjon diffusjonssveising av sintrete uoksiderte keramiske komponenter, og strukturer bestaende av uoksidert keramikk med en somlos sammenfoyning

To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…