To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…
Inventor / Author Profile
Rendtel Andreas Dr
26Total Forward Citations
2Indexed Patents
2Patent H-Index
Frequent Co-Inventors: Kayser Ursula Meschke Frank Dr
To bond two components of a sintered and non-oxide ceramic material, they are joined together by diffusion welding in a hot press in a protective gas atmosphere. They are heated to a temperature of at least 1600 [deg] C, preferably >= 1800 [deg] C and especially >= 2000…