WO 2013/002112 A1#16722166 Most Cited · 6 citations0.5/yr · PR 2.15PendingWO · Application
Process for producing solder joint with improved reliability

A highly reliable joint which is inhibited, during operation, from suffering a volume change accompanying phase transformation or suffering troubles such as strains or cracks caused by a volume change is rendered possible with an Sn-Cu solder alloy by regulating the cooling…

US 2014030140 A1#33810940 Most Cited · 3 citations0.2/yr · PR 1.00PendingUS · Application
Solder alloy

A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.

WO 2012/137901 A1#39864129 Most Cited · 2 citations0.1/yr · PR 1.02PendingWO · Application
Solder alloy

This solder alloy contains Al and/or Al 2 O 3 in the amount of 0.006-0.15 wt% in an Sn-Cu hypereutectic area. In addition, this solder alloy comprises Cu in the amount of 0.7-7.6 wt%, and Al and/or Al 2 O 3 in the amount of 0.006-0.5 wt%, with the remainder being Sn. Preferably,…

WO 2015/053114 A1#42224831 Most Cited · 2 citations0.2/yr · PR 0.96PendingWO · Application
Low-melting brazing filler metal

The purpose of the present invention is to inhibit the formation of Cu 3 SnIMC in a lead-free, low-melting, Sn-Cu based brazing filler metal and thereby provide a low-melting brazing filler metal which can attain improved joint reliability. This brazing filler metal is an Sn-Cu…

CN 103,547,407 A#48830840 Most Cited · 1 citations0.1/yr · PR 0.89ActiveCN · Utility
Solder alloy

The invention provides a solder alloy which contains Al and/or Al2O3 in the amount of 0.006-0.15 wt% in an Sn-Cu hypereutectic area. In addition, this solder alloy comprises Cu in the amount of 0.7-7.6 wt%, and Al and/or Al2O3 in the amount of 0.006-0.5 wt%, with the remainder…

US 9,999,945 B2#61548769 Most Cited · 1 citations0.1/yr · PR 0.75ActiveUS · Utility
Solder alloy

A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.

EP 2,695,701 A1#102232192 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Solder alloy

This solder alloy contains Al and/or Al 2 O 3 in the amount of 0.006-0.15 wt% in an Sn-Cu hypereutectic area. In addition, this solder alloy comprises Cu in the amount of 0.7-7.6 wt%, and Al and/or Al 2 O 3 in the amount of 0.006-0.5 wt%, with the remainder being Sn. Preferably,…