Disclosed is a solder join in which the occurrence of cracking is suppressed. A joint is produced from a solder alloy comprising 0.01 to 7.6 wt% of Cu and 0.001 to 6 wt% of Ni, with the remainder being Sn. The alloy allows the maximum ranges of the Cu content and the Ni content.…
Nishimura Tetsuro
Ternary leadless solder comprising l-2 wt.% of Cu, 0.002-l wt.% of Ni, and Sn for the rest, wherein the contents of Cu and Ni are preferably 0.3-0.7 wt.% and 0.04-0.l wt.% respectively, a method of adding Ni to a Sn-Cu alloy and a method of adding Cu to a Sn-Ni alloy being…
Disclosed is a solder jointed article in which the occurrence cracking is suppressed. Specifically disclosed is a lead-free solder alloy comprising 0.01 to 7.6 wt% of Cu and 0.001 to 6 wt% of Ni, with the remainder being Sn. The alloy allows the maximum ranges of the Cu content…
This method controls a copper density in a dip solder bath holding a molten solder alloy containing at least copper as an essential composition thereof during a dip soldering step of one of a printed circuit board with a surfaced copper foil and a component part having a copper…
A solder free from lead for additional supply to control the Cu concentration and Ni concentration in solder bath which sharply vary depending upon the particularity of post-process; and a method of regulating the Cu concentration and Ni concentration in solder bath under such…
A highly reliable joint which is inhibited, during operation, from suffering a volume change accompanying phase transformation or suffering troubles such as strains or cracks caused by a volume change is rendered possible with an Sn-Cu solder alloy by regulating the cooling…
A method by which the amount of nickel contained in an alloy having a composition represented by Sn-X-Ni can be regulated. The method of nickel concentration regulation comprises adding phosphorus to Sn-X-Ni in a molten state (wherein X is one or more elements selected from the…
A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.
A solder joint manufactured of an alloy essentially composed of 0.01-7.6 wt % Cu, 0.001-6 wt % Ni, and the remaining of Sn. Each of Cu and Ni has a maximum concentration range. The lower limit of the range of Ni is 0.01 wt % and preferably 0.03 wt %. The upper limit of the range…
A method by which the amount of nickel contained in an alloy having a composition represented by Sn—X—Ni can be regulated. The method of nickel concentration regulation comprises adding phosphorus to Sn—X—Ni in a molten state (wherein X is one or more elements selected from the…
A method by which the amount of nickel contained in an alloy having a composition represented by Sn—X—Ni can be regulated. The method of nickel concentration regulation comprises adding phosphorus to Sn—X—Ni in a molten state (wherein X is one or more elements selected from the…
Generation of voids is suppressed by means of a conventional apparatus without using attached apparatuses, such as a pressure reducing apparatus, in solder bonding wherein a BGA ball solder and a cream solder are used. The ball solder and the cream solder have a relationship…
A flux for soldering and a soldering paste containing the flux are provided, the paste suffering no viscosity change with time and neither filming nor becoming non-flowable. The soldering paste has satisfactory applicability, printability, and soldering properties. The flux for…
Disclosed is a negative electrode structure for a lithium ion secondary battery having high stability. Specifically disclosed is a negative electrode structure for a lithium ion secondary battery, which comprises an electrode composed of Cu or an alloy mainly composed of Cu and…
Provided is a wire solder with high tensile strength and pull cut resistance. An apparatus for feeding the wire solder is also provided. The wire solder has an extended wire solder and a core wire having a higher tensile strength than the wire solder. The core wire is made of…
This solder alloy contains Al and/or Al 2 O 3 in the amount of 0.006-0.15 wt% in an Sn-Cu hypereutectic area. In addition, this solder alloy comprises Cu in the amount of 0.7-7.6 wt%, and Al and/or Al 2 O 3 in the amount of 0.006-0.5 wt%, with the remainder being Sn. Preferably,…
The present invention addresses the problem of providing, at low cost, a lead-free solder alloy which has high reliability and excellent joining characteristics and which is suitable for mounting a microscopic electronic component. This lead-free solder alloy has a composition…
An apparatus for depositing and separating excess copper dissolved in molten lead-free solder containing tin as the main element is provided. An apparatus 1 deposits excess copper in the molten lead-free solder as an intermetallic compound and separates it from the molten…
Provided is an apparatus for feeding wire solder with high tensile strength and pull cut resistance. The wire solder has an extended wire solder and a core wire having a higher tensile strength than the wire solder. The apparatus for feeding the wire solder comprises a wire…
The present invention provides a lead-free solder alloy having high reliability and excellent solder bonding properties and suited for the mounting of micronized electronic components at low cost. The lead-free solder alloy according to the present invention has a composition…
The present invention provides a lead-free solder alloy having high reliability and excellent solder bonding properties and suited for the mounting of micronized electronic components at low cost. The lead-free solder alloy according to the present invention has a composition…
A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.
A lead-free solder characterized as comprising 0.1 to 2 wt % of Cu, 0.002 to 1 wt % of Ni with the residue being Sn. The solder preferably contains Cu in an amount of 0.3 to 0.7 wt %, and more preferably it contains Cu in an amount of 0.3 to 0.7 wt % and Ni in an amount of 0.04…
Provided is a solder with high tensile strength and pull cut resistance. The wire solder has an extended wire solder and a core wire having a higher tensile strength than the wire solder. The wire solder has a single or multiple strands bound together. The wire solder is…
An apparatus for depositing and separating excess copper dissolved in molten lead-free solder containing tin as the main element is provided. An apparatus 1 deposits excess copper in the molten lead-free solder as an intermetallic compound and separates it from the molten…