A process is described for preparing polyisobutene having a content of terminal vinylidene groups of at least 75 mol % by polymerizing isobutene or isobutenic hydrocarbon mixtures in the liquid phase in the presence of a boron trifluoride complex catalyst of the composition (BF…
Perner Thomas
The invention relates to a method for producing polyisobutene with an average molecular weight that ranges between 400 and 50,000 and a methylidene group content of more than 50 mol % by the polymerisation of a reaction mixture containing isobutene in the presence of a catalyst…
Periodic variation of at least one process parameter with time is used in a low-pressure process for the production of polyolefin (co)polymers with a wide mol. wt. distribution and/or polydispersity of comonomer content.
A synthetic resin which carries basic nitrogen groups and is water-dilutable by protonation with acid is obtainable by reacting (A) an epoxy resin having an average molecular weight M n of from 200 to 6,000 and on average from 1.5 to 3.0 epoxy groups per molecule with (B) a…
The invention relates to a method for drying and degassing polyolefins. The polymerisation matter leaving a polymerisation reactor is contacted with a degassing medium and relaxed at the same time. According to the invention, the monomer to be polymerised is used as the…
The invention relates to a method for producing low halogen polyisobutenes. The inventive method is characterized in that isobutene is polymerized in the presence of a catalyst which contains a halogenated Lewis acid, the catalyst is removed and/or deactivated, and the…
A synthetic resin which carries basic nitrogen groups and is water-dilutable by protonation with an acid, containing (A) a chain-extended, amine-modified epoxy resin obtainable by reacting (a1) an epoxy resin having an average molecular weight Mn of from 300 to 6,000 and on…
A process is described for preparing polyisobutene having a low halogen content, in which isobutene is polymerized in the presence of a catalyst which comprises a halogenated Lewis acid, the catalyst is removed and/or deactivated, and the resulting polyisobutene is contacted…
The invention relates to a method for producing polyisobutene containing at least 75 mol- % terminal vinylidene groups. Said method consists in polymerising an isobutene or hydrocarbon mixture containing isobutene in the liquid phase in the presence of a boron trifluoride…
Production of polyisobutene with number average molecular weight Mn 400-50000 and over 50 mole-% methylidene groups by polymerization of a reaction mixture containing isobutene in the presence of a catalyst containing boron trifluoride, is carried out at least partly in the…
A binder which is water-dilutable on protonation with acid and obtainable by a reaction of (A) an epoxy resin having an average molecular weight of from 300 to 6,000 and on average from 1.5 to 3.0 epoxide groups per molecule and (B) from 20 to 30 mol %, based on the amount of…
A process is described for preparing polyisobutene having a low halogen content, in which isobutene is polymerized in the presence of a catalyst which comprises a halogenated Lewis acid, the catalyst is removed and/or deactivated, and the resulting polyisobutene is contacted…
The invention relates to a method for producing low halogen polyisobutenes. The inventive method is characterized in that isobutene is polymerized in the presence of a catalyst which contains a halogenated Lewis acid, the catalyst is removed and/or deactivated, and the…
A process is described for preparing polyisobutene having a content of terminal vinylidene groups of at least 75 mol % by polymerizing isobutene or isobutenic hydrocarbon mixtures in the liquid phase in the presence of a boron trifluoride complex catalyst of the composition (BF…
A binder which is water-dilutable on protonation with acid and obtainable by a reaction of (A) an epoxy resin having an average molecular weight of from 300 to 6,000 and on average from 1.5 to 3.0 epoxide groups per molecule and (B) from 20 to 30 mol %, based on the amount of…
A synthetic resin which carries basic nitrogen groups and is water-dilutable by protonation with an acid, containing (A) a chain-extended, amine-modified epoxy resin obtainable by reacting (a 1 ) an epoxy resin having an average molecular weight M n of from 300 to 6,000 and on…
A synthetic resin which carries basic nitrogen groups and is water-dilutable by protonation with acid is obtainable by reacting (A) an epoxy resin having an average molecular weight M n of from 300 to 6,000 and on average from 1.5 to 3.0 epoxy groups per molecule with (B) a…
The binders for cathodic electrocoating which become water-thinnable on protonation with an acid and are thermally crosslinkable in the presence of an acid, contain by covalent bonding the groups <IMAGE> where R is a C2-C18-alkyl, a cycloalkyl or an aralkyl group which…
A synthetic resin which carries basic nitrogen groups and is water-dilutable by protonation with acid is obtainable by reacting (A) an epoxy resin having an average molecular weight M n of from 300 to 6,000 and on average from 1.5 to 3.0 epoxy groups per molecule with (B) a…
The invention relates to a method for drying and degassing polyolefins in which the polymerization product leaving a polymerization reactor is brought into contact with a degassing medium and simultaneously decompressed. The degassing medium employed according to the invention…
A binder which is water-dilutable on protonation with acid and obtainable by a reaction of (A) an epoxy resin having an average molecular weight of from 300 to 6,000 and on average from 1.5 to 3.0 epoxide groups per molecule and (B) from 20 to 30 mol %, based on the amount of…
The synthetic resin can be protonated by means of acid and diluted by means of water and is obtainable by reaction of A) an epoxy resin having a mean molecular weight Mn of from 300 to 6000 and an average of from 1.5 to 3.0 epoxide groups per molecule with B) a secondary…
The present invention relates to aqueous dispersions of copolymers which contain epoxide groups, obtainable by copolymerisation in the aqueous phase of A) 50 to 96 % by weight of a vinyl ester, B) 4 to 50 % by weight of an alpha , beta -monoolefinically unsaturated epoxide…
An apparatus for the intensive degassing of polyvinyl chloride-containing dispersions comprising a polymerization reactor (1), a cooling device (2), and a vacuum unit (3), where the polymerization reactor (1) contains a steam inlet (4) in the lower half, and the polymerization…