Bimodal polyethylene blends are made from a high-molecular-weight ethylene copolymer and a low-molecular-weight ethylene homo- or copolymer and have a melt flow rate MFR 190/21.6 of from 6 to 14 g/10 min, a density of from 0.94 to 0.97 g/cm 3 , an environmental-stress-cracking…
Deckers Andreas
In a process for the polymerization or copolymerization of ethylenically unsaturated monomers in the presence of polymerization initiators which decompose to form free radicals in a continuously operated polymerization apparatus comprising a fresh gas feed line, a precompressor,…
PCT No. PCT/EP93/01222 Sec. 371 Date Nov. 22, 1994 Sec. 102(e) Date Nov. 22, 1994 PCT Filed May 17, 1993 PCT Pub. No. WO93/24561 PCT Pub. Date Dec. 9, 1993.An expandable styrene polymer comprising a) from 0 to 90% by weight of a styrene polymer or styrene copolymer other than b)…
The invention relates to a method for producing ether carboxylates.
Proceso para preparar ácido cianhídrico por deshidratación catalítica de formamida gaseosa, donde la deshidratación de la formamida se acopla con una reacción exotérmica por el reactor usado en la deshidratación que comprende dos caminos de fluidos separados los cuales están…
A moulding composition comprising, based on the sum of A, B, C and D, A: from 5 to 50% by weight of a methyl methacrylate polymer A comprising, based on A, A1: from 80 to 100% by weight of units of methyl methacrylate (A1) and A2: up to 20% by weight of units of an alkyl…
A particulate graft polymer comprising a graft base A comprising, based on A, A11: from 75 to 99.8 % by weight of at least one elastomeric polymer-forming alkyl acrylate A11 having up to 8 carbon atoms in the alkyl radical, A12: from 0.1 to 5 % by weight of at least one…
Moulding compositions which are resistant to stress cracking, essentially comprising A) from 49 to 99 % by weight of a polymer obtainable by polymerisation of a C1-C20-alkyl ester of methacrylic or acrylic acid, or mixtures of such esters, B) from 0.95 to 50 % by weight of a…
PCT No. PCT/EP93/01222 Sec. 371 Date Nov. 22, 1994 Sec. 102(e) Date Nov. 22, 1994 PCT Filed May 17, 1993 PCT Pub. No. WO93/24561 PCT Pub. Date Dec. 9, 1993.An expandable styrene polymer comprising a) from 0 to 90% by weight of a styrene polymer or styrene copolymer other than b)…
Expandable styrene polymers (I) for elastic polystyrene (PS) foam contain: (a) 50-90 wt.% PS and/or styrene copolymer contg. at least 50% styrene; (b) 5-30 wt.% styrene-soluble elastomer(s), (c) 5-20 wt.% styrene-contg. block copolymer(s); (d) 1-15 wt.% (w.r.t. a+b+c)…
Preparation of ethylene polymers (A) by a high pressure process involves dissolving radical initiator(s) in ketone(s) (I); compressing; dosing the mixture to the polymerization reactor in one or more portions; and carrying out polymerization. Preparation of ethylene polymers (A)…
The invention relates to a method for producing hydrocyanic acid by the thermolysis of gaseous formamide in a reactor in the presence of a catalyst, wherein a) the catalyst (i) is an aluminum oxide catalyst, containing - 90 to 100 wt%, preferably 99 to 100 wt%, of aluminum oxide…
A moulding composition comprising, based on the sum of A, B, C and D, A: from 5 to 50% by weight of a methyl methacrylate polymer A comprising, based on A, A1: from 80 to 100% by weight of units of methyl methacrylate (A1) and A2: up to 20% by weight of units of an alkyl…
A copolymer (I) based on ethylene and vinyl formate units is claimed. Also claimed are fuel and motor fuel compositions containing (I).
The invention relates to a method for producing hydrocyanic acid by catalytic dehydration of gaseous formamide, the catalytic dehydration being carried out in a tubular reactor at a certain temperature profile.
A process is disclosed for preparing ethylene polymers with a molecular weight Mw (weight average) lower than 20,000 g/mole at temperatures in a range from 200 to 280 °C and pressures in a range from 1000 to 3500 bars in the presence of a catalyst system. The catalyst system…