Outlet weir of tank is lower than inlet and electrolyte is forced to flow in alternately downward and upward paths between anodes and cathodes at velocities in excess of 10 feet per minute and preferably 20 to 100 feet per minute. Cathodes (or anodes) are spaced from bottom of…
Inventor / Author Profile
Norman Telfer E
89Total Forward Citations
8Indexed Patents
5Patent H-Index
Frequent Co-Inventors: Stolk Douglas A
A tough abrasion-resistant refrigeration-hardenable white cast iron containing as its essential alloying constituents about 2.5% to about 3.5% carbon, about 2.5% to about 3.5% manganese, about 12% to about 22% chromium, about 1% to about 2% silicon, about 1.5% to about 3.0%…
An abrasion-resistant high-chromium type of alloyed white iron, which can be hardened and toughened by refrigeration at sub-zero temperatures, containing as its essential alloying constituents about 2.6% to about 3.6% carbon, about 12% to about 22% chromium, about 0.5% to about…