Outlet weir of tank is lower than inlet and electrolyte is forced to flow in alternately downward and upward paths between anodes and cathodes at velocities in excess of 10 feet per minute and preferably 20 to 100 feet per minute. Cathodes (or anodes) are spaced from bottom of…
Assignee / Organization
Norman Telfer E
66Total Forward Citations
4Indexed Patents
16Avg Citations / Patent
3Portfolio H-Index
Key Inventors: Norman Telfer E
An abrasion-resistant high-chromium type of alloyed white iron, which can be hardened and toughened by refrigeration at sub-zero temperatures, containing as its essential alloying constituents about 2.6% to about 3.6% carbon, about 12% to about 22% chromium, about 0.5% to about…