Patents
US 5,716,909 A#18211430 Most Cited · 6 citations0.2/yr · PR 1.49ExpiredUS · Utility
Process for increasing the pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings
Inventors: Majewski Peter, Petzow Guenter, Aldinger Fritz, Hettich Bernhard, Elschner SteffenAssignee: Hoechst AgFiled 1996-10-01 · Granted 1998-02-10

Process for increasing the pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings, which comprises heating the pure-phase 2212 phase of a Bi-Sr-Ca-Cu-O ceramic molding under pure oxygen or an oxygen-containing gas for from 1 to 40 minutes to a temperature of from 825°…

EP 0,630,873 A1#23917983 Most Cited · 4 citations0.1/yr · PR 1.53PendingEP · Application
Process for enhancing the pinning strength of a superconducting Bi-Pb-Sr-Ca-Cu-O ceramic

To increase the pinning force of superconductive Bi-Pb-Sr-Ca-Cu-O material, the Pb2223 ceramic is heated to a temperature of preferably from 865 to 870 DEG C in an oxygen-containing atmosphere for a period of from 1 to 60 minutes. This produces precipitates of (Sr,Ca)14Cu24O41-x…

US 5,250,509 A#29591096 Most Cited · 3 citations0.1/yr · PR 1.29ExpiredUS · Utility
Bismuth-containing superconducting material and process for producing it
Inventors: Hettich Bernhard, Majewski Peter, Schulze Klaus, Petzow GuenterAssignee: Hoechst AgFiled 1992-02-20 · Granted 1993-10-05

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of Bi y Ca 2 Sr 2 Cu 3 O x , where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical…

DE 10,246,780 A1#41879471 Most Cited · 2 citations0.1/yr · PR 0.97PendingDE · Application
Production of silicon carbide, useful as abrasive and polish, in metallurgy and for ceramic, or mixture with aluminum involves heating graphite with basic or ultrabasic rock, amorphous silica or silicate containing aluminum
Inventors: Majewski PeterAssignee: Max Planck GesellschaftFiled 2002-10-08

In process (A) for producing silicon carbide by heating a silica component and graphite, basic or ultrabasic rock with a silica content at most 70 wt.% is used as silica component Independent claims are also included for other processes as follows: (B) production of silicon…

DE 3,414,485 A1#38294893 Most Cited · 2 citations0.1/yr · PR 1.07PendingDE · Application
Hollow drill for removing multi-legged, electronic components which are soldered into printed-circuit boards
Inventors: Majewski PeterAssignee: Majewski PeterFiled 1984-04-17

According to the methods which were previously known to me for releasing multi-legged, electronic components from printed-circuit boards, this is very expensive, is partially position-dependent or can even be implemented technically only with difficulty. Using the hollow drill…

EP 0,504,840 A2#59529330 Most Cited · 1 citations0.0/yr · PR 0.77PendingEP · Application
Superconducting material containing bismuth and process for its production

Die Erfindung betrifft ein oxodkeramisches supraleitendes Material, das Wismut, Strontium, Kalzium und Kupfer enthält, mit einer Bruttozusammensetzung von BiyCa2Sr2Cu3Ox, bei der y eine Zahl von 2,35 bis 2,6 bedeutet und x etwa 10 bis 12. Das Material zeigt eine…

AU 1,300,492 A#149930662 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Bismuth-containing superconducting material and process for producing it

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

AU 649,114 B2#68645629 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Bismuth-containing superconducting material and process for producing it
Inventors: Hettich Bernhard, Majewski Peter, Schulze Klaus, Petzow GunterAssignee: Hoechst AgFiled 1992-03-18 · Granted 1994-05-12

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

CA 2,063,313 A1#123654978 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Bismuth-containing superconducting material and process for producing it

Abstract of the disclosure Bismuth-containing superconducting material and process for producing it The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y…

CA 2,111,166 A1#71646974 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Process for increasing the pinning force of superconducting bi-sr-ca-cu-o ceramic moldings

Abstract: Process for increasing the pinning force of supercon-ducting Bi-Sr-Ca-Cu-O ceramic moldings Process for increasing the pinning force of supercon-ducting Bi-Sr-Ca-Cu-O ceramic moldings, which comprises heating the pure-phase 2212 phase of a Bi-Sr-Ca-Cu-O ceramic molding…

CN 1,092,052 A#149233071 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
Increase the method for pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings
Inventors: Majewski Peter, Petzow Guenter, Aldinger FritzAssignee: Hoechst AgFiled 1993-12-10

The invention provides a kind of method that increases pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings, this method is included in pure oxygen or the oxygen-containing gas pure phase 2212 heat phase to 825-900 of Bi-Sr-Ca-Cu-O ceramic moulded goods ℃, 1-40…

DE 3,437,801 A1#101804298 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Device for desoldering multi-legged electronic components
Inventors: Majewski PeterAssignee: Majewski PeterFiled 1984-10-16

The previous methods known to me for detaching multi-legged electronic components from printed-circuit boards are very expensive, are in some cases location-dependent or else can be technically implemented only with difficulty. Using the device invented by me which…

DE 3,444,602 A1#150669223 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Tool for desoldering multi-legged electronic components
Inventors: Majewski PeterAssignee: Majewski PeterFiled 1984-12-07

According to the methods which have been known by me until now for detaching multi-legged electronic components from printed-circuit boards, this process is very expensive, to some extent position- dependent or can also be technically implemented only with difficulty. Using the…

DE 4,108,869 A1#89155621 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Verfahren zur herstellung eines bismut enthaltenden supraleitenden materials

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

DE 59,208,988 D1#65540828 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Wismut enthaltendes supraleitendes Material und Verfahren zu seiner Herstellung
Inventors: Hettich Bernhard Dr, Majewski Peter Dr, Schulze Klaus Dr, Petzow Guenter ProfAssignee: Hoechst AgFiled 1992-03-18 · Granted 1997-12-04

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

DK 0,504,840 T3#134383331 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDK · Utility
Bismuthholdigt supraledende materiale og fremgangsmåde til dets fremstilling.
Inventors: Hettich Bernhard Dr, Majewski Peter Dr, Schulze Klaus Dr, Petzow Guenter ProfAssignee: Hoechst AgFiled 1992-03-18 · Granted 1998-05-25

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

EP 0,504,840 A3#122702500 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Superconducting material containing bismuth and process for its production

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…

EP 0,602,507 A1#98255506 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Process for the enhancement of the Pinning force of superconducting bismuth-strontium-calcium-copper-oxygen ceramic bodies

Process for enhancing the pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic shaped bodies, characterised in that the phase-pure 2212 phase of a Bi-Sr-Ca-Cu-O ceramic shaped body is heated for from 1 to 40 minutes under pure oxygen or under an oxygen-containing gas to a…

ES 2,109,955 T3#75313530 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Material superconductor que contiene bismuto y procedimiento para su preparacion.
Inventors: Hettich Bernhard Dr, Majewski Peter Dr, Schulze Klaus Dr, Petzow Gunter ProfAssignee: Hoechst AgFiled 1992-03-18 · Granted 1998-02-01

LA INVENCION CONCIERNE A UN MATERIAL SUPRACONDUCTIVO OXOCERAMICO QUE CONTIENE BISMUTO, ESTRONCIO, CALCIO Y COBRE, CON UNA COMPOSICION BRUTA DE BIYCA2SR2CU3OX, EN LA QUE Y SIGNIFICA UN NUMERO ENTRE 2,35 Y 2,6 Y X 10 A 12. EL MATERIAL PRESENTA UNA TEMPERATURA DE PICO TC POR ENCIMA…

GR 3,025,432 T3#108165047 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredGR · Utility
Superconducting material containing bismuth and process for its production

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of BiyCa2Sr2Cu3Ox, where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical temperature T…