Patents
DE 4,343,742 A1#8053404 Most Cited · 12 citations0.4/yr · PR 3.45PendingDE · Application
Turning disc mill
Inventors: Hettich Bernhard G Dipl IngAssignee: Krupp Polysius AgFiled 1993-12-21

The disc mill has a counterweight system formed by a single counterweight (9) in an axial extension, in the immediate vicinity of the barrel (2) for the material. One driven eccentric shaft (4) is made to run synchronously with the other eccentric shafts via the counterweight.…

EP 0,327,044 A1#9107352 Most Cited · 11 citations0.3/yr · PR 2.62PendingEP · Application
Superconductor and process for its production

A description is given of superconducting materials containing Bi, Sr, Ca and Cu and of a process for producing them from the metal oxides within a range which is given by the overall composition Bia(Sr,Ca)bCu6Ox, where a = 3 - 24 and b = 3.23 - 24, with a Sr/Ca atomic ratio of…

US 4,141,660 A#14429479 Most Cited · 7 citations0.1/yr · PR 2.44ExpiredUS · Utility
Printer for data-processing machine having single operator station
Inventors: Bommersheim Hans, Hettich Bernhard, Keller Helmut, Moser Werner, Tauchert KlausAssignee: Kienzle Apparate GmbhFiled 1977-11-21 · Granted 1979-02-27

A data-processing machine having a single operator station is provided with a printer comprising a supply holder on the front of the machine next to the operator station for holding a form band, a support on the machine next to the station with an upwardly concave surface, and a…

DE 3,311,786 A1#16236449 Most Cited · 6 citations0.1/yr · PR 6.17PendingDE · Application
Method for generating a deflection current for a cathode-ray tube
Inventors: Hettich Bernhard, Tenten WilfriedAssignee: Licentia GmbhFiled 1983-03-31

In order to correct deflection errors, it is proposed to superimpose a correction current on the deflection current, which correction current is formed from an actual value signal of a sensor in comparison with a desired value.

US 5,716,909 A#18211430 Most Cited · 6 citations0.2/yr · PR 1.49ExpiredUS · Utility
Process for increasing the pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings
Inventors: Majewski Peter, Petzow Guenter, Aldinger Fritz, Hettich Bernhard, Elschner SteffenAssignee: Hoechst AgFiled 1996-10-01 · Granted 1998-02-10

Process for increasing the pinning force of superconducting Bi-Sr-Ca-Cu-O ceramic moldings, which comprises heating the pure-phase 2212 phase of a Bi-Sr-Ca-Cu-O ceramic molding under pure oxygen or an oxygen-containing gas for from 1 to 40 minutes to a temperature of from 825°…

DE 3,803,530 A1#22523838 Most Cited · 4 citations0.1/yr · PR 5.94PendingDE · Application
Superconductor and process for the production thereof

Black crystal compositions having the gross composition Bia(Sr, Ca)bCu6Ox, with a = 3-12 and b = 6-12, having an atom ratio Sr/Ca of from 1:9 to 9:1, an atom ratio Bi:(Sr + Ca) of 0.3-1.3, can be produced if a mixture of the oxides of bismuth, calcium, strontium and copper or…

EP 0,441,268 A1#24432647 Most Cited · 4 citations0.1/yr · PR 1.43PendingEP · Application
Process for the production of shaped bodies of superconductive oxide ceramic material
Inventors: Kalz Hans-juergen Dr, Hettich Bernhard DrAssignee: Hoechst AgFiled 1991-02-02

In the process for the production of shaped bodies of superconductive oxide-ceramic material having high critical current densities, a superconductive oxide-ceramic powder is used which contains spherical particles (a) having a mean particle size smaller than 10 mu m and…

EP 0,630,873 A1#23917983 Most Cited · 4 citations0.1/yr · PR 1.53PendingEP · Application
Process for enhancing the pinning strength of a superconducting Bi-Pb-Sr-Ca-Cu-O ceramic

To increase the pinning force of superconductive Bi-Pb-Sr-Ca-Cu-O material, the Pb2223 ceramic is heated to a temperature of preferably from 865 to 870 DEG C in an oxygen-containing atmosphere for a period of from 1 to 60 minutes. This produces precipitates of (Sr,Ca)14Cu24O41-x…

EP 0,481,337 A1#30514298 Most Cited · 3 citations0.1/yr · PR 1.21PendingEP · Application
Superconducting composition and process for its production

A description is given of a black superconducting material having the overall composition Bi4 (Sr, Ca)yCuzO delta , where z = 2-3, y = 4-6 and Sr/Ca is 1:1 to 10:1. It contains at least 10% by weight of a superconducting phase of the general formula Bi4+x-(Sr, Ca)5-xCu3O4+ delta…

US 5,250,509 A#29591096 Most Cited · 3 citations0.1/yr · PR 1.29ExpiredUS · Utility
Bismuth-containing superconducting material and process for producing it
Inventors: Hettich Bernhard, Majewski Peter, Schulze Klaus, Petzow GuenterAssignee: Hoechst AgFiled 1992-02-20 · Granted 1993-10-05

The invention relates to an oxide-ceramic superconducting material which contains bismuth, strontium, calcium and copper, having an overall composition of Bi y Ca 2 Sr 2 Cu 3 O x , where y is an integer from 2.35 to 2.6 and x is about 10 to 12. The material has a critical…

AU 608,946 B2#36859726 Most Cited · 2 citations0.1/yr · PR 1.14ExpiredAU · Utility
Superconductor and process for its preparation
Inventors: Schnering Hans-georg Von, Becker Winfried, Schwarz Martin, Hettich Bernhard, Hartweg MartinAssignee: Hoechst AgFiled 1989-02-03 · Granted 1991-04-18

A description is given of superconducting materials containing Bi, Sr, Ca and Cu and of a process for producing them from the metal oxides within a range which is given by the overall composition Bia(Sr,Ca)bCu6Ox, where a = 3 - 24 and b = 3.23 - 24, with a Sr/Ca atomic ratio of…

DE 4,005,282 A1#38760114 Most Cited · 2 citations0.1/yr · PR 1.05PendingDE · Application
Verfahren zur herstellung stabfoermiger koerper aus hochtemperatursupraleitendem material

Process for producing a rod-like superconductive body by zone melting of an oxidic material containing bismuth, strontium, calcium and copper with the composition of a superconductor and heating a solid sample by a laser, in which a block-shaped, pressed or sintered body of any…

EP 0,571,885 A1#39961357 Most Cited · 2 citations0.1/yr · PR 1.01PendingEP · Application
Slip from high temperature super-conductor precursors for the production of green ceramic sheets and processing thereof

A slip from high-temperature superconducting precursor material for green ceramic sheets is described. As ceramic starting material for the sheet-casting process, the slip contains a precursor powder which consists of the elements Bi, Sr, Ca, Cu and O, and which is prepared by…

EP 0,602,508 A2#36934529 Most Cited · 2 citations0.1/yr · PR 1.14PendingEP · Application
Process for the homopolymerisation and copolymerisation of 1-olefins

In order to prepare poly-1-olefins, in particular polyethylene, a supported Ziegler catalyst is used whose transition-metal component has been prepared by reacting a magnesium alkoxide dispersion whose particle size is from 100 to 3000 nm simultaneously with various compounds of…

US 5,703,021 A#43303042 Most Cited · 2 citations0.1/yr · PR 0.93ExpiredUS · Utility
Process for making high temperature Bi-Sr-Ca-Cu oxide superconductor
Inventors: Von Schnering Hans-georg, Becker Winfried, Schwarz Martin, Hettich Bernhard, Hartweg MartinAssignee: Hoechst AgFiled 1995-06-07 · Granted 1997-12-30

A description is given of superconducting substances having a content of Bi, Sr, Ca and Cu, and of processes for their preparation from the metal oxides within a range which is specified by the overall composition Bi a (Sr,Ca) b -Cu 6 O x , where a=3-24 and b=3.23-24, with an…

AU 2,958,889 A#48166310 Most Cited · 1 citations0.0/yr · PR 0.93ExpiredAU · Utility
Superconductor and process for its preparation

A description is given of superconducting materials containing Bi, Sr, Ca and Cu and of a process for producing them from the metal oxides within a range which is given by the overall composition Bia(Sr,Ca)bCu6Ox, where a = 3 - 24 and b = 3.23 - 24, with a Sr/Ca atomic ratio of…