Patents
US 4,528,231 A#1401527 Most Cited · 40 citations1.0/yr · PR 5.48ExpiredUS · Utility
Slip and wear resistant flooring and compositions and a method for producing same
Inventors: Lund ThoreAssignee: Skf Steel Eng AbFiled 1983-05-05 · Granted 1985-07-09

Wear and slip resistant floors are described comprising a suitable substrate and a surface layer comprising a synthetic resin, preferably polyester, as the matrix and containing uniformly distributed therein a mixed waste material derived from a steel grinding operation and…

US 6,149,743 A#3696043 Most Cited · 22 citations0.8/yr · PR 3.36ExpiredUS · Utility
Method of complete bainite hardening
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1998-07-21 · Granted 2000-11-21

A method of complete bainite hardening of steel for use in bearings and other load carrying components, wherein bainite transformation is performed at a temperature just above the martensite formation temperature, transforming 25%-99% of the austenite into bainite at said…

EP 0,896,068 A1#4755673 Most Cited · 18 citations0.7/yr · PR 5.26PendingEP · Application
Bainite hardening
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1998-07-28

A method of complete bainite hardening of steel for use in bearings and other load carrying components, wherein bainite transformation is performed at a temperature just above the martensite formation temperature, transforming 25 - 99 % of the austen-ite into bainite at said…

DE 19,821,797 C1#5629617 Most Cited · 16 citations0.6/yr · PR 3.87ExpiredDE · Utility
Hardened steel parts used for roller bearing parts
Inventors: Hengerer Frank Dr, Lund ThoreAssignee: Skf GmbhFiled 1998-05-15 · Granted 1999-07-08

Hardened steel parts are produced from an air hardening steel by air cooling from the hot working temperature and simultaneously calibrating. A hardened steel part is produced by heating an air hardening steel to above 1100 deg C, hot working at up to the A1 temperature, air…

WO 2010/134867 A1#9567829 Most Cited · 11 citations0.7/yr · PR 1.86PendingWO · Application
Bearing component
Inventors: Lund Thore, Strandell IngemarAssignee: Skf Ab, Lund ThoreFiled 2010-05-20

Bearing component (10) containing steel that comprises, by weight, 10-30 ppm Ca,, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide inclusions.

EP 1,094,124 A2#11623803 Most Cited · 9 citations0.4/yr · PR 2.10PendingEP · Application
Super clean steel
Inventors: Lund ThoreAssignee: Ovako Steel AbFiled 2000-05-19

A super clean steel for use in objects subjected to heavy loads in all directions, such as in fuel injection pumps or bearings, comprising, in weight, O max. 7 ppm, Ti max. 15 ppm, and S between about 8 ppm and about 12 ppm, and having a K1(total) value according to DIN 50 602…

US 2011223818 A1#12064915 Most Cited · 9 citations0.6/yr · PR 1.72PendingUS · Application
Bearings for Pod Propulsion System

An improved bearing assembly includes one unique shaft washer ( 158 ) rather than using separate forward and aft shaft washers as in the prior art; a slight lengthening of the forward roller ( 174 ) as compared to the aft roller ( 176 ); an increase in the diameter of the…

US 4,973,368 A#11944016 Most Cited · 9 citations0.2/yr · PR 1.83ExpiredUS · Utility
Method of manufacturing steel elements designed to withstand high stress, such as roller bearing elements
Inventors: Lund ThoreAssignee: Ovako Steel AbFiled 1989-07-20 · Granted 1990-11-27

Steel elements designed to withstand high stress, such as roller bearing elements, are produced by using a steel which has substantially eutectoid composition, a such a steel billet being plasticly formed, without prior soft-annealing, at a temperature just above the A1…

CN 1,211,634 A#13371758 Most Cited · 8 citations0.3/yr · PR 1.85ExpiredCN · Utility
Vanadium alloyed bearing steel
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1998-07-31

An improved vanadium alloyed bearing steel having the following alloying elements, in weight-%, 0.60 to 1.10% C, 0 to 2.10%, preferably, 0.40 to 2.10% Si, 0 to 2.00%, preferably, 0.10 to 1.00% Mn, 0 to 2.00%, preferably, 0.50 to 2.00% Ni, 0 to 2.00% Cr, 0 to 0.75%, preferably, 0…

US 5,122,337 A#13941083 Most Cited · 8 citations0.2/yr · PR 1.44ExpiredUS · Utility
Steel intended for highly stressed structural members with high demands for ductility and fatigue resistance
Inventors: Lund Thore, Munther Hans-akeAssignee: Ovako Steel AbFiled 1990-12-26 · Granted 1992-06-16

Steel is described which is improved by dissolving components of the steel that oppose its workability into a ferrite phase of the steel, and by combining components of the steel that impart desirable properties to it with carbon to form carbides. The steel is useful for highly…

EP 0,943,694 A1#15666931 Most Cited · 7 citations0.3/yr · PR 1.59PendingEP · Application
A method for the manufacture of components made of steel
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1999-03-15

A method for the manufacture of components made of steel subject to heavy stress, load and/or wear, such as rolling bearing elements, starting from a steel having an austenite carbon content at hot forming temperature of about 800 - 1100°C of 0.55-0.85 wt%, hot forming of the…

US 6,176,948 B1#14828094 Most Cited · 7 citations0.3/yr · PR 1.99ExpiredUS · Utility
Method for the manufacture of components made of steel
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1999-03-16 · Granted 2001-01-23

A method for the manufacture of components made of steel subject to heavy stress, load and/or wear, such as rolling bearing elements, hot forming components of a steel having an austenite carbon content at a hot forming temperature of about 800-1100° C. of 0.55-0.85 wt %, above…

CN 103,547,696 A#17498468 Most Cited · 6 citations0.5/yr · PR 1.69ActiveCN · Utility
Improved bearing steel
Inventors: Lund Thore, Ryden Karin, Strandell Ingemar, Hallberg JoakimAssignee: Skf AbFiled 2012-05-16

The invention relates to a bearing steel comprising at least 0.6 wt.% carbon, 0.007 wt.% or less phosphorus and optionally other alloying element, the balance being iron or iron and impurities. The invention also relates to a bearing made of the bearing steel.

CN 103,237,914 A#19661524 Most Cited · 5 citations0.4/yr · PR 1.89ActiveCN · Utility
Steel and component for high temperature joining process
Inventors: Lund ThoreAssignee: Skf AbFiled 2011-12-06

Steel suitable for high temperature joining processes, in particular for components with high demands on fatigue properties and toughness, such as bearing components, comprising the following composition in weight-%: 0.5-0.8C, 0-0.15Si, 0-1.0Mn, 0.01-2.0Cr, 0.01-1.0Mo,…

CN 1,214,368 A#20298198 Most Cited · 5 citations0.2/yr · PR 1.62ExpiredCN · Utility
Method of complete bainite hardening of steel
Inventors: Lund Thore, Larsson Staffan, Oelund PatrikAssignee: Ovako Steel AbFiled 1998-07-31

A method of complete bainite hardening of steel for use in bearings and other load carrying components, wherein bainite transformation is performed at a temperature just above the martensite formation temperature, transforming 25%-99% of the austenite into bainite at said…

US 2014026674 A1#21434304 Most Cited · 5 citations0.4/yr · PR 1.39PendingUS · Application
Method for fatigue assessment of rolling bearing
Inventors: Lund Thore, Ryden KarinAssignee: Lund Thore, Ryden KarinFiled 2012-03-28

The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…

CN 103,748,449 A#22803247 Most Cited · 4 citations0.3/yr · PR 2.26ActiveCN · Utility
Method for fatigue assessment of rolling bearing
Inventors: Lund Thore, Ryden KarinAssignee: Skf AbFiled 2012-03-28

The present invention relates to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…

FR 2,636,076 A1#25934320 Most Cited · 4 citations0.1/yr · PR 1.25PendingFR · Application
Procede de fabrication d'elements en acier concus pour resister a des contraintes elevees, tels que des elements de roulements a rouleaux
Inventors: Lund ThoreAssignee: Ovako Steel AbFiled 1989-09-01

L'invention concerne un procédé de fabrication d'éléments en acier conçus pour résister à des contraintes élevées. Ce procédé comprend l'utilisation d'un acier qui présente une composition sensiblement eutectode, le formage d'une billette à partir de cet…

US 2012063944 A1#26015857 Most Cited · 4 citations0.3/yr · PR 1.25PendingUS · Application
Bearing component
Inventors: Lund Thore, Strandell IngemarAssignee: Lund Thore, Strandell IngemarFiled 2010-05-20

Bearing component ( 10 ) containing steel that comprises, by weight, 10-30 ppm Ca, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide inclusions.

US 9,074,970 B2#25798690 Most Cited · 4 citations0.4/yr · PR 1.27ActiveUS · Utility
Method for fatigue assessment of rolling bearing
Inventors: Lund Thore, RydÉn KarinAssignee: Lund Thore, RydÉn KarinFiled 2012-03-28 · Granted 2015-07-07

The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…

WO 2012/002869 A1#24603386 Most Cited · 4 citations0.3/yr · PR 1.40PendingWO · Application
Flash-butt welded bearing component
Inventors: Lund Thore, Recina ViktorAssignee: Skf Ab, Lund ThoreFiled 2011-05-27

Bearing component (10) comprising steel and at least one flash butt weld joint. The steel comprises, by weight, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide…

WO 2012/082040 A1#23433884 Most Cited · 4 citations0.3/yr · PR 1.68PendingWO · Application
Steel and component intended for high temperature joining processes
Inventors: Lund ThoreAssignee: Skf Ab, Lund ThoreFiled 2011-12-06

Steel for a high temperature joining process suitable, in particular for components intended for applications with high demands on fatigue and toughness properties, such as bearing components, comprising the following composition in weight-%: 0.5-0.8 C, 0- 0.15 Si, 0-1.0 Mn,…

WO 2012/138275 A1#22512049 Most Cited · 4 citations0.3/yr · PR 8.37PendingWO · Application
Method for fatigue assessment of rolling bearing
Inventors: Lund Thore, Ryden KarinAssignee: Skf Ab, Lund ThoreFiled 2012-03-28

The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…

WO 2012/158089 A1#28696378 Most Cited · 3 citations0.2/yr · PR 1.44PendingWO · Application
Improved bearing steel

The present invention relates to a bearing steel comprising at least 0.6 percent by weight of carbon, 0.007 percent by weight or less of phosphorous, and optionally other alloying element(s); the balance being iron, or iron and impurities. The present invention also relates to a…