Bearing component (10) containing steel that comprises, by weight, 10-30 ppm Ca,, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide inclusions.
Lund Thore
The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…
Bearing component ( 10 ) containing steel that comprises, by weight, 10-30 ppm Ca, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide inclusions.
The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…
Bearing component (10) comprising steel and at least one flash butt weld joint. The steel comprises, by weight, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide…
Steel for a high temperature joining process suitable, in particular for components intended for applications with high demands on fatigue and toughness properties, such as bearing components, comprising the following composition in weight-%: 0.5-0.8 C, 0- 0.15 Si, 0-1.0 Mn,…
The present invention related to a method, and an apparatus arrangement, for determining a fatigue limit for rolling contact initiated fatigue of a rolling bearing. The method comprises running a rolling bearing while being exerted to a load which generates sub-surface…
The present invention relates to a bearing steel comprising at least 0.6 percent by weight of carbon, 0.007 percent by weight or less of phosphorous, and optionally other alloying element(s); the balance being iron, or iron and impurities. The present invention also relates to a…
Method for heat treating a steel component ( 28, 36 ) comprising the steps of: a) carbonitriding the steel component ( 28, 36 ) at a temperature of 930-970° C., b) cooling the steel component ( 28, 36 ), d) re-heating the steel component ( 28, 36 ) to a temperature of 780-820°…
The present invention relates to a bearing steel comprising at least 0.6 percent by weight of carbon, 0.007 percent by weight or less of phosphorous, and optionally other alloying element(s); the balance being iron, or iron and impurities. The present invention also relates to a…
Bearing component ( 10 ) comprising steel and at least one flash butt weld joint. The steel comprises, by weight, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide…
Method for manufacturing at least one steel ring blank (18) or ring segment blank, which comprises steps of forging steel into a sleeve (16), and cutting said at least one steel ring blank (18) or ring segment blank from the forged sleeve (16).
Method for manufacturing at least one steel ring blank (18) or ring segment blank, which comprises steps of forging steel into a sleeve (16), and cutting said at least one steel ring blank (18) or ring segment blank from the forged sleeve (16).
Bearing component ( 10 ) comprising steel and at least one flash butt weld joint. The steel comprises, by weight, max 20 ppm S and max 15 ppm O and in that said steel includes sulphide inclusions and less than 5% of the sulphide inclusions contain encapsulated or embedded oxide…
Steel for a high temperature joining process suitable, in particular for components intended for applications with high demands on fatigue and toughness properties, such as bearing components, comprising the following composition in weight-%: 0.5-0.8 C, 0- 0.15 Si, 0-1.0 Mn,…
Method for heat treating a steel component (28, 36) comprising the steps of: a) carbonitriding the steel component (28, 36) at a temperature of 930-970°C, b) cooling the steel component (28, 36), d) re-heating the steel component (28, 36) to a temperature of 780-820°C and d)…