The invention concerns the use of a WC—Co cutting metal alloy for a component or a tool insert, which is shaped from a corresponding cutting metal blank by means of an electrical discharge processing method. The WC fraction in the carbide phase of the cutting metal alloy is more…
Lackner Andreas
Electrical components (ECs) (17) for transmitting signals/data built into a crane link to a communications interface (18) for setting up an on-line signal/data transmission path (30) to an electronic calculating device/computer (19) like a personal computer (20). A…
A hard metal grade powder is produced from hard material, metal binder, and non-water-soluble pressing aid components, by forming a slurry containing the components and pure water as a liquid phase and then drying the slurry. Here, the hard material and metal binder components…
A hard metal grade powder is produced from hard material, metal binder, and non-water-soluble pressing aid components, by forming a slurry containing the components and pure water as a liquid phase and then drying the slurry. Here, the hard material and metal binder components…
A hard metal granulate is produced by wet milling and spray drying in a spray tower using pure water as the liquid phase. The spray tower is configured and operated in such a way that a ratio of the quantity of water added via the slurry (in liters per hour) to tower volume (in…
The invention relates to a method for producing a hard metal projection made of hard material portions, binding metal portions and water-soluble pressing auxiliary agent portions by drying a wet slurry, which contains the constituents and pure water as the liquid phase.…
PROBLEM TO BE SOLVED: To obtain WC particles having a specific average primary particle size and not having a different phase capable of being proved by an X-ray diffraction method by heating a substance to be carburized up to a specific process temperature, charging a specific…
The invention concerns a gas carburizing method for production of fine-grained tungsten carbide (WC) powder in installations for fluidized bed reaction starting from free-flowing tungsten or tungsten oxide-containing powder with an average particle size d50>10 mum in a single…
The run-out positions (10,11,12) of the cable strands (2,3,4) from the drums (7) or rollers (9) form an equilateral triangle (D) and the centre lines of the downwardly guided cable strands determine a three-sided pyramid (P) with its point (S) directed downwards. The point of…
The invention relates to a method for producing a hard metal granulated material by carrying out wet milling and spray drying inside a spray tower -1- while using pure water as the liquid phase. According to the invention, the spray tower -1- is configured and operated in such a…
Fine grain tungsten carbide (WC) powder is made by gas carburization of non-granulated tungsten (W) or W oxide-containing powder in a fluidized bed at elevated temperature using a carbon-containing process gas comprising either (i) 10-100 vol. % carbon oxides COx and a remainder…
Hard metal alloy contains a carbide phase with more than 90 wt.% tungsten carbide and 8-15 wt.% cobalt binder phase in which a metal additive is completely dissolved. The additive is selected from one or more of rhenium, germanium, gallium, iridium, osmium, palladium, silver,…
A hard metal granulate is produced by wet milling and spray drying in a spray tower using pure water as the liquid phase. The spray tower is configured and operated in such a way that a ratio of the quantity of water added via the slurry (in liters per hour) to tower volume (in…
The invention relates to a method for producing a hard metal granulated material by carrying out wet milling and spray drying inside a spray tower -1- while using pure water as the liquid phase. According to the invention, the spray tower -1- is configured and operated in such a…
Use of a carbide hard metal alloy based on tungsten carbide with a binder phase containing 4-12 wt.% cobalt and 0.01-0.8 wt.% iridium for cutting inserts of rock drills is new. Preferred Features: The hard metal alloy contains at least 90 wt.% tungsten carbide or 6-9 wt.%…
The device has gripping units (19) fastened to an elongate carrier (11) and arranged in series. Each gripping unit is provided with a movable gripping arm that has a shape of a circular arc and is displaceable along the circular arc shape. The gripping arm is supported over a…
The invention relates to a method for producing a hard metal projection made of hard material portions, binding metal portions and water-soluble pressing auxiliary agent portions by drying a wet slurry, which contains the constituents and pure water as the liquid phase.…
The invention relates to a method for producing a hard metal projection made of hard material portions, binding metal portions and water-soluble pressing auxiliary agent portions by drying a wet slurry, which contains the constituents and pure water as the liquid phase.…
The hanger has a control device (23) power and communication connected with a crane controller (22). The control device exhibits control electronics for generation of a signal from angle of deflection (32) of a control lever. The control device is movably attached at an end…
The invention relates to a method for the production of metal carbide powders from powdered carburization material i.e. metal, reducible metal compounds and/or carbon. Microwave technology is used to produce the temperature required and to add heat required for initiation of the…
Die Erfindung betrifft die Verwendung einer WC-Co-Hartmetall-Legierung für ein Bauteil oder einen Werkzeugeinsatz, die mittels funkenerosiver Bearbeitungsverfahren aus entsprechendem Hartmetall-Rohling geformt werden. Der WC-Anteil an der Karbidphase der Hartmetall-Legierung…
In the present invention, there is disclosed a method of producing hard metal-based refractory formulation wherein the formulation is produced from hard material, metal binder, and non-water-soluble pressing aid component, by forming a slurry containing the above-indicated…
The run-out positions (10,11,12) of the cable strands (2,3,4) from the drums (7) or rollers (9) form an equilateral triangle (D) and the centre lines of the downwardly guided cable strands determine a three-sided pyramid (P) with its point (S) directed downwards. The point of…
The invention relates to a process for producing a hard metal batch by drying a wet slurry - 3 - which is produced by wet-milling the hard material and binder metal fractions desired in the finished batch to the desired grain size, using water as liquid phase. According to the…
The invention relates to a method for producing a hard metal stock by drying a wet sludge (3), which is obtained by the wet grinding of the hard substance and binding metal to the desired particle size, in the quantities required for the finished stock, using water as the liquid…