Method for producing hard metal granulate

4Forward Citations (#27390771 Global)
0.2/yrCitation Velocity (#34961074 Global)
1.00Citation PageRank (#41598130 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A hard metal granulate is produced by wet milling and spray drying in a spray tower using pure water as the liquid phase. The spray tower is configured and operated in such a way that a ratio of the quantity of water added via the slurry (in liters per hour) to tower volume (in m 3 ) is between 0.5 and 1.8 and in that a maximum of 0.17 kg of slurry is atomized per m 3 of incoming drying gas. The slurry has a solid particle concentration within a range of 65-85% by weight. Under these conditions, the addition of a water-soluble, long-chain polyglycol to the slurry prior to spraying previously required in order to prevent oxidation of the hard metal granulate is no longer necessary.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a hard metal granulate, which comprises: wet milling hard material and binding metal components desired in the hard metal granulate and preparing a sprayable slurry with water as a liquid phase and having a solid particle concentration within a range of 65-85% by weight; introducing the slurry into a spray tower spray-drying the slurry in a gas stream having a gas inlet temperature of substantially 160° to 220° C. and a gas exit temperature in a range of substantially 85° to 130° C., to convert the slurry to granular form; wherein the slurry is sprayed and dried substanti